Polymer Property : Izod Impact, Notched = 2.46 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.46 J/cm

@Temperature -30.0 °C
4.61 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer (Europe-Africa-Middle East)
PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supplied by ..
Izod Impact, Notched 2.46 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
4.60 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Elastoblend® PA6 GF33 IM3 BK 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac..
Izod Impact, Notched 2.46 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
4.60 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES HiFill® PP CO GF30 CC 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc.
Izod Impact, Notched 2.46 J/cm

@Thickness 3.17 mm
4.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS
VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS).
Izod Impact, Notched 2.46 J/cm

@Thickness 3.17 mm
4.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS
VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS).
Izod Impact, Notched 2.46 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
4.60 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES HiFill® PP CO GF20 CC 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc.
Izod Impact, Notched 2.46 J/cm

@Temperature 23.0 °C
4.61 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Verton RV008ESV_GY7E072 PA 66
Preliminary data for 40% long glass fiber filled, single color pellet gray, PA66This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 2.46 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
4.60 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Chi Mei Kibilac® PW-978B ASA, High Heat
Acrylonitrile/Styrene/AcrylateInformation provided by Calsak Corporation
Izod Impact, Notched 2.46 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
4.61 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Diamond Polymers DIAMALOY GLY 7510 High Heat ASA Weatherable Polymer
Diamaloy GLY 7510 resin is a high gloss, high heat and high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. This product is rated f1 by UL and be customed..
Izod Impact, Notched 2.46 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
4.60 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Chi Mei Kibilac® PW-978D ASA, High Heat  (discontinued **)
Acrylonitrile/Styrene/AcrylateInformation provided by Calsak Corporation