Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.70 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.18 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87775 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 1.70 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.18 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ISO 180/4A |
Polimeri Europa Sinkral® PD L 322 ABS Resin Sinkral PD L 322 by continuous mass, is a general purpose, high flow injection molding grade having good impact resistance coupled with an excellent gloss.Applications: Widely used in the small and.. |
|||
Izod Impact, Notched | 1.70 J/cm @Temperature 23.0 °C |
3.18 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS (Asia Pacific) PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 1.70 J/cm @Temperature 23.0 °C |
3.18 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS (Europe-Africa-Middle East) PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 1.70 J/cm @Temperature 23.0 °C |
3.18 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS (Europe-Africa-Middle East) Reinforced PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 1.70 J/cm @Temperature -40.0 °C |
3.18 ft-lb/in @Temperature -40.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl PX1404 PPE+PS PPE+PS blend. High Heat. FDA compliant with restrictions. Injection Molding and Extrusion.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 1.70 J/cm @Temperature -40.0 °C |
3.18 ft-lb/in @Temperature -40.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Valox® 365 PET Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031".This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 1.70 J/cm @Temperature 23.0 °C |
3.18 ft-lb/in @Temperature 73.4 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® T-663G50A MXD66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 1.70 J/cm @Temperature 23.0 °C |
3.18 ft-lb/in @Temperature 73.4 °F |
Practical Use; ASTM-D256 |
Toyobo GLAMIDE® T-669VGB Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 1.70 J/cm @Temperature -40.0 °C |
3.18 ft-lb/in @Temperature -40.0 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® TY-181GC Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 1.70 J/cm @Temperature 23.0 °C |
3.18 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP KUR 1060 GFC Polypropylene, 30% Glass Filled PP copolymer 30% chemically coupled glass fiberElastomer modified, good impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.70 J/cm @Temperature 23.0 °C |
3.18 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D256 |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**) Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 1.70 J/cm @Temperature 23.0 °C |
3.18 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Americas region. |