Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.92 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
7.35 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HI100K ABS, High Impact Feature: Injection Molding, High Impact, Good ProcessingApplication: Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 3.92 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 7.35 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL EI5002 PP Description: Injection Molding, PP, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 9002-88-4Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 3.92 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 7.35 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL HI4352L PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, Good Dimensional Stability, High ImpactApplication: Automotive Exterior (Sill Side Molding, Door Garnish)CAS: 9003-07-0, 26221-73-8 and 14807-96-6Inform.. |
|||
Izod Impact, Notched | >= 3.92 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
>= 7.35 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LUPOY SC1004L PC, High Impact Description: Injection Molding, PC, General Purpose, High Flow, High Impact, Chemical ResistanceApplication: Mobile Phone HousingInformation provided by LG Chemical |
|||
Izod Impact, Notched | 3.92 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
7.35 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical RS656H ABS, Chemical Resistance to Cyclopentane Feature: Extrusion Molding, General Purpose, Chemical Resistance to CyclopentaneApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 3.92 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
7.35 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical RS657L ABS, Chemical Resistance to Cyclopentane, Low Specific Gravity Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 3.92 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
7.35 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical RS800M ABS, High Modulus, Chemical Resistance to HCFC Feature: Extrusion Molding, High Modulus, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 3.92 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 7.35 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL MC4352 PP+Rubber+MF Description: Injection Molding, PP+Rubber+MF, Good Dimensional Stability, Scratch resistance, Good Weatherability, High ImpactApplication: Automotive Exterior (Sill Side Molding, Door Garnish)CAS: 9.. |
|||
Izod Impact, Notched | 3.92 J/cm @Thickness 6.35 mm |
7.35 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® HA-1011 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 3.92 J/cm @Thickness 6.35 mm |
7.35 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1041 PC/ABS, Unreinforced Metal Plating Grade High flow PC/ABS material that can be used for automobile R/G door handleInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 3.92 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
7.35 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 3.92 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
7.35 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1089 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 3.92 J/cm @Thickness 6.35 mm |
7.35 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® HA-1011 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 3.92 J/cm @Thickness 6.35 mm |
7.35 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1041 PC/ABS, Unreinforced Metal Plating Grade High flow PC/ABS material that can be used for automobile R/G door handleInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 3.92 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
7.35 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1041G PC/ABS, Unreinforced Metal Plating Grade Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 3.92 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
7.35 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 3.92 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
7.35 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1089 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 3.92 J/cm @Temperature 23.0 °C |
7.35 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
SCG Chemicals EL-Leneâ„¢ H1000P High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stabilityRecommended Applications: Water pipes, conduit, sewage drainage pipesInformation provided by SCG Chemicals |
|||
Izod Impact, Notched | 3.92 J/cm @Thickness 3.20 mm |
7.35 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron IM11GMS ABS Injection Molding Grade High Rigidity, High Impact, High Chemical ResistanceInformation provided by Bhansali |
|||
Izod Impact, Notched | 3.92 J/cm @Thickness 6.40 mm |
7.35 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron IMC-45 ABS-PC Alloy ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali |
|||
Izod Impact, Notched | 3.92 J/cm @Thickness 6.40 mm |
7.35 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron SE32H Extrusion ABS Very High Impact, Better Flow and Sheet/Pipe/Profile applicationInformation provided by Bhansali |
|||
Izod Impact, Notched | 3.92 J/cm @Thickness 6.40 mm |
7.35 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron BL60 Impact modifier for PVC Impact modifier for PVC, White powderInformation provided by Bhansali |
|||
Izod Impact, Notched | 3.92 J/cm @Thickness 6.40 mm |
7.35 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron SE32H Extrusion ABS Very High Impact, Better Flow and Sheet/Pipe/Profile applicationInformation provided by Bhansali |
|||
Izod Impact, Notched | 3.92 J/cm @Temperature 23.0 °C |
7.35 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
E-Polymers SEPAZ® LC40 PP Copolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Izod Impact, Notched | 3.92 J/cm @Temperature -30.0 °C |
7.35 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
E-Polymers SEPAZ® LC40 PP Copolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Izod Impact, Notched | 3.92 J/cm @Thickness 3.20 mm |
7.35 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron IM11GMS ABS Injection Molding Grade High Rigidity, High Impact, High Chemical ResistanceInformation provided by Bhansali |
|||
Izod Impact, Notched | 3.92 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
7.35 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical MA201 ABS, Low Gloss Feature: Injection Molding, Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 3.92 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
7.35 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1041G PC/ABS, Unreinforced Metal Plating Grade Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 3.92 J/cm @Thickness 6.40 mm |
7.35 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron BL60 Impact modifier for PVC Impact modifier for PVC, White powderInformation provided by Bhansali |
|||
Izod Impact, Notched | 3.92 J/cm @Thickness 6.40 mm |
7.35 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron IMC-45 ABS-PC Alloy ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali |