Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.1569 J/cm @Thickness 3.20 mm |
4.0408 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron HR-59 ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.1569 J/cm @Thickness 6.40 mm |
4.0408 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron HR-59(M) ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.1569 J/cm @Thickness 6.40 mm |
4.0408 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron HR-60 ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.1569 J/cm @Thickness 6.40 mm |
4.0408 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron HR-60 ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.1569 J/cm @Thickness 3.20 mm |
4.0408 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron HR-59 ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.1569 J/cm @Thickness 6.40 mm |
4.0408 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron HR-59(M) ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |