Mechanical Properties Metric English Comments
Izod Impact, Notched 4.54 J/cm

@Temperature -40.0 °C
8.50 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Oxford Polymers 604-I Polycarbonate/ABS Alloy
Polycarbonate/ABS AlloyInformation provided by Oxford Polymers.
Izod Impact, Notched 4.54 J/cm

@Thickness 3.17 mm,
Temperature -20.0 °C
8.50 ft-lb/in

@Thickness 0.125 in,
Temperature -4.00 °F
ASTM D256
Techmer ES Elastoblend® PA6 IM 7040 MB
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier, Nucleating Agent and LubricantFeatures: Heat Stabilized, Impact Modified, Nucleated and LubricatedInformation pro..
Izod Impact, Notched 4.54 J/cm

@Thickness 3.17 mm,
Temperature -20.0 °C
8.50 ft-lb/in

@Thickness 0.125 in,
Temperature -4.00 °F
ASTM D256
Techmer ES Elastoblend® PA6 IM 7050
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier, Nucleating Agent and LubricantFeatures: Heat Stabilized, Impact Modified, Nucleated and LubricatedInformation pro..
Izod Impact, Notched 4.54 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
8.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Axiall UV-6685 Rigid PVC, Molding
Georgia Gulf UV 6685 is a high flow PVC compound designed for thin wall parts and multi-cavity molds. It is ideally suited for a variety of parts requiring resistance to outdoor UV degradation.Info..