Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 206 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 206 GPa

@Temperature 316 °C
29900 ksi

@Temperature 601 °F
(heat treated at 1121°C (2050°F), water quenched plate)
Haynes Ultimet® alloy, 1.6 mm sheet
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Modulus of Elasticity 206 GPa

@Temperature 316 °C
29900 ksi

@Temperature 601 °F
(heat treated at 1121°C (2050°F), water quenched plate)
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Modulus of Elasticity 206 GPa

@Temperature 316 °C
29900 ksi

@Temperature 601 °F
(heat treated at 1121°C (2050°F), water quenched plate)
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, SMAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Modulus of Elasticity 206 GPa

@Temperature 316 °C
29900 ksi

@Temperature 601 °F
(heat treated at 1121°C (2050°F), water quenched plate)
Haynes Ultimet® alloy, 12.7-50.8 mm bar
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Modulus of Elasticity 206 GPa

@Temperature 316 °C
29900 ksi

@Temperature 601 °F
(heat treated at 1121°C (2050°F), water quenched plate)
Haynes Ultimet® alloy, 19.1 mm thick plate, SMAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Modulus of Elasticity 206 GPa

@Temperature 316 °C
29900 ksi

@Temperature 601 °F
(heat treated at 1121°C (2050°F), water quenched plate)
Haynes Ultimet® alloy, 6.3-38.1 mm plate
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Modulus of Elasticity 206 GPa

@Temperature 316 °C
29900 ksi

@Temperature 601 °F
(heat treated at 1121°C (2050°F), water quenched plate)
Haynes Ultimet® alloy, aged 1000 hours at 204°C (400°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Modulus of Elasticity 206 GPa

@Temperature 316 °C
29900 ksi

@Temperature 601 °F
(heat treated at 1121°C (2050°F), water quenched plate)
Haynes Ultimet® alloy, aged 1000 hours at 316°C
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Modulus of Elasticity 206 GPa

@Temperature 316 °C
29900 ksi

@Temperature 601 °F
(heat treated at 1121°C (2050°F), water quenched plate)
Haynes Ultimet® alloy, aged 1000 hours at 427°C (800°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Modulus of Elasticity 206 GPa

@Temperature 316 °C
29900 ksi

@Temperature 601 °F
(heat treated at 1121°C (2050°F), water quenched plate)
Haynes Ultimet® alloy, aged 1000 hours at 538°C (1000°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Modulus of Elasticity 206 GPa

@Temperature 316 °C
29900 ksi

@Temperature 601 °F
(heat treated at 1121°C (2050°F), water quenched plate)
Haynes Ultimet® alloy, aged 1000 hours at 649°C (1200°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Modulus of Elasticity 206 GPa

@Temperature 316 °C
29900 ksi

@Temperature 601 °F
(heat treated at 1121°C (2050°F), water quenched plate)
Haynes Ultimet® alloy, aged 1000 hours at 760°C (1400°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Modulus of Elasticity 206 GPa

@Temperature 316 °C
29900 ksi

@Temperature 601 °F
(heat treated at 1121°C (2050°F), water quenched plate)
Haynes Ultimet® alloy, aged 1000 hours at 871°C (1600°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Modulus of Elasticity 206 GPa

@Temperature 316 °C
29900 ksi

@Temperature 601 °F
(heat treated at 1121°C (2050°F), water quenched plate)
Haynes Ultimet® alloy, aged 1000 hours at 982°C
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Modulus of Elasticity 206 GPa

@Temperature 316 °C
29900 ksi

@Temperature 601 °F
(heat treated at 1121°C (2050°F), water quenched plate)
Haynes Ultimet® alloy, all-weld metal, GMAW weld (short)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Modulus of Elasticity 206 GPa

@Temperature 316 °C
29900 ksi

@Temperature 601 °F
(heat treated at 1121°C (2050°F), water quenched plate)
Haynes Ultimet® alloy, all-weld metal, GMAW weld (spray)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Modulus of Elasticity 206 GPa

@Temperature 316 °C
29900 ksi

@Temperature 601 °F
(heat treated at 1121°C (2050°F), water quenched plate)
Haynes Ultimet® alloy, all-weld metal, GTAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Modulus of Elasticity 206 GPa

@Temperature 316 °C
29900 ksi

@Temperature 601 °F
(heat treated at 1121°C (2050°F), water quenched plate)
Haynes Ultimet® alloy, all-weld metal, SMAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Modulus of Elasticity 206 GPa

@Temperature 316 °C
29900 ksi

@Temperature 601 °F
(heat treated at 1121°C (2050°F), water quenched plate)
Haynes Ultimet® alloy, mill annealed
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Modulus of Elasticity 206 GPa

@Temperature 316 °C
29900 ksi

@Temperature 601 °F
(heat treated at 1121°C (2050°F), water quenched plate)
Haynes Ultimet® alloy, plate, GMAW weld (short)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Modulus of Elasticity 206 GPa

@Temperature 316 °C
29900 ksi

@Temperature 601 °F
(heat treated at 1121°C (2050°F), water quenched plate)
Haynes Ultimet® alloy, plate, GMAW weld (spray)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..