Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 188 GPa @Temperature 600 °C |
27300 ksi @Temperature 1110 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Bar, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Modulus of Elasticity | 188 GPa @Temperature 600 °C |
27300 ksi @Temperature 1110 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Modulus of Elasticity | 188 GPa @Temperature 538 °C |
27300 ksi @Temperature 1000 °F |
|
Haynes R-41 alloy, Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ.. |
|||
Modulus of Elasticity | 188 GPa @Temperature 538 °C |
27300 ksi @Temperature 1000 °F |
|
Haynes R-41 alloy, 1.27 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, air cooled, aged 16 hours at 760°C (1400°F) Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ.. |
|||
Modulus of Elasticity | 188 GPa @Temperature 538 °C |
27300 ksi @Temperature 1000 °F |
|
Haynes R-41 alloy, sheet 0.762-2.54 mm exclusive, 30 minutes at 1066°C, air cooled, aged 16 hours at 760°C (1400°F) Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ.. |
|||
Modulus of Elasticity | 188 GPa @Temperature 538 °C |
27300 ksi @Temperature 1000 °F |
|
Haynes R-41 alloy, sheet 0.762-2.54 mm exclusive, 30 minutes at 1121°C, air cooled, aged 16 hours at 899°C Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ.. |
|||
Modulus of Elasticity | 188 GPa @Temperature 600 °C |
27300 ksi @Temperature 1110 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Modulus of Elasticity | 188 GPa @Temperature 600 °C |
27300 ksi @Temperature 1110 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Sheet, Cold Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Modulus of Elasticity | 188 GPa @Temperature 600 °C |
27300 ksi @Temperature 1110 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Modulus of Elasticity | 188 GPa @Temperature 500 °C |
27300 ksi @Temperature 932 °F |
|
Special Metals INCONEL® alloy N06230 Ni-Cr-W-Mo Alloy INCONEL® alloy N06230 (UNS N06230 / W.Nr. 2.4733) is a carbide strengthened nickel-chromium-tungsten-molybdenum alloy with an exceptional combination of strength, stability, and resistance to cor.. |
|||
Modulus of Elasticity | 188 GPa @Temperature 600 °C |
27300 ksi @Temperature 1110 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Plate, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe.. |
|||
Modulus of Elasticity | 188 GPa @Temperature 600 °C |
27300 ksi @Temperature 1110 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe.. |
|||
Modulus of Elasticity | 188 GPa @Temperature 538 °C |
27300 ksi @Temperature 1000 °F |
|
Haynes R-41 alloy, Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications include .. |
|||
Modulus of Elasticity | 188 GPa @Temperature 400 °C |
27300 ksi @Temperature 752 °F |
Dynamic |
Haynes 617 Nickel Alloy Plate Haynes 617 alloy is a nickel-chromium-cobalt-molybdenum alloy with a good combination of metallurgical stability, strength, and oxidation resistance at high temperatures. The alloy is readily formed.. |