Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Total Energy | 59.6 J/cm @Temperature 23.0 °C |
0.112 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
PolyOne Geon™ HTX Ultra LA426 Gray 2382 Polyvinyl Chloride Alloy (PVC Alloy) Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical propert.. |
|||
Dart Drop Total Energy | 59.6 J/cm @Temperature 23.0 °C |
0.112 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
PolyOne Geon™ HTX Ultra LA426 Tan 3725 Polyvinyl Chloride Alloy (PVC Alloy) Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical propert.. |
|||
Dart Drop Total Energy | 60.0 J/cm @Temperature 23.0 °C |
0.112 ft-lb/mil @Temperature 73.4 °F |
|
Mapal Plastics Maplon Type H Polypropylene Sheet Properties : Good resistance to low temperatures, Moderate stress whitening, Suitable for die cutting, Corona treated on both sides for offset and screen printing.Applications : Stationery, Printing.. |