Polymer Property : Dart Drop Total Energy = 0.333 ft-lb/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Total Energy 178 J/cm

@Temperature 23.0 °C
0.333 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
PolyOne Geon™ Vinyl Rigid Extrusion 87416 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Dart Drop Total Energy 178 J/cm

@Temperature 23.0 °C
0.333 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
PolyOne Geon™ Vinyl Rigid Extrusion L0189 Polyvinyl Chloride, Rigid (PVC, Rigid)
All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high ..
Dart Drop Total Energy >= 178 J/cm

@Temperature 23.0 °C
>= 0.333 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
PolyOne Geon™ Vinyl Rigid Extrusion L7005 Polyvinyl Chloride, Rigid (PVC, Rigid)
Geon L7005 is recommended for whites and light pastel colors only.Note: Physical properties based on L7005 tan 3210 sample.Information provided by PolyOne
Dart Drop Total Energy 178 J/cm

@Temperature 23.0 °C
0.333 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
PolyOne Geon™ Vinyl Rigid Extrusion L7007 Polyvinyl Chloride, Rigid (PVC, Rigid)
Geon L7007 is recommended for whites and light pastel colors only.Geon L7007 is a higher gloss version of L7005.Information provided by PolyOne
Dart Drop Total Energy 178 J/cm

@Temperature 23.0 °C
0.333 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
PolyOne Geon™ Vinyl Rigid Extrusion L7416 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Dart Drop Total Energy 178 J/cm

@Temperature 23.0 °C
0.333 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
PolyOne Geon™ Vinyl Rigid Extrusion L7801 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Dart Drop Total Energy 178 J/cm

@Temperature 23.0 °C
0.333 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
PolyOne Geon™ HTX Ultra LA425 Polyvinyl Chloride Alloy (PVC Alloy)
Optimum for Black and Darker Colors below 50L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Ductile/Brittle transition as measured by Instrumented Impact is 5 de..
Dart Drop Total Energy >= 178 J/cm

@Temperature 23.0 °C
>= 0.333 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
PolyOne Geon™ HTX Ultra LA426 Black 2880 Polyvinyl Chloride Alloy (PVC Alloy)
Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA426 Black 2880.Information provided by PolyOne
Dart Drop Total Energy 178 J/cm

@Temperature 23.0 °C
0.333 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
PolyOne Geon™ HTX Ultra LA426 Gray 2382 Polyvinyl Chloride Alloy (PVC Alloy)
Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical propert..
Dart Drop Total Energy 178 J/cm

@Temperature 23.0 °C
0.333 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
PolyOne Geon™ HTX Ultra LA426 Tan 3725 Polyvinyl Chloride Alloy (PVC Alloy)
Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical propert..
Dart Drop Total Energy >= 178 J/cm

@Temperature 23.0 °C
>= 0.333 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
PolyOne Geon™ L4605 Green 5765 Polyvinyl Chloride, Semi-Rigid (PVC, Semi-Rigid)
Information provided by PolyOne
Dart Drop Total Energy >= 178 J/cm

@Temperature 23.0 °C
>= 0.333 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
PolyOne Geon™ L4605 Ivory 3098 Polyvinyl Chloride, Semi-Rigid (PVC, Semi-Rigid)
Information provided by PolyOne
Dart Drop Total Energy 178 J/cm

@Temperature 23.0 °C
0.333 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
PolyOne Geon™ Vinyl Cellular E8202 Polyvinyl Chloride, Rigid (PVC, Rigid)
All physicals were measured on an actual extruded part of a shutter profile.High rate inward foam applications.Density range .55-.70.Information provided by PolyOne
Dart Drop Total Energy 178 J/cm

@Temperature 23.0 °C
0.333 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
PolyOne Geon™ Vinyl Dry Blend E1500 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Dart Drop Total Energy 178 J/cm

@Temperature 23.0 °C
0.333 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
PolyOne Geon™ Vinyl Dry Blend E1501 Polyvinyl Chloride, Rigid (PVC, Rigid)
VSI FLAMMABILITY:Burn Length (0.040 in Bar)ASTM D635 0* IN.Burn Time (0.040 in Bar) ASTM D635 0* Sec.*Extinguished before 25 MM starting ref mark.Information provided by PolyOne
Dart Drop Total Energy 178 J/cm

@Temperature 23.0 °C
0.333 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
PolyOne Geon™ Vinyl Dry Blend E7000 Polyvinyl Chloride, Rigid (PVC, Rigid)
60 degree gloss comparisons: Geon E7000 is 47-49;Geon E7456 is 40-49;Geon E7130 is 38-43;Geon E7370 is 26-31Information provided by PolyOne
Dart Drop Total Energy 178 J/cm

@Temperature 23.0 °C
0.333 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
PolyOne Geon™ Vinyl Dry Blend E7001 Polyvinyl Chloride, Rigid (PVC, Rigid)
60 degree gloss comparisons: Geon E7001 is 27-29; Geon E7456 is 40-49; Geon E7130 is 38-43; Geon E7370 is 26-31Information provided by PolyOne
Dart Drop Total Energy 178 J/cm

@Temperature 23.0 °C
0.333 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
PolyOne Geon™ Vinyl Dry Blend E7456 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Dart Drop Total Energy >= 178 J/cm

@Temperature 23.0 °C
>= 0.333 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
PolyOne Geon™ Vinyl Rigid Extrusion L6256 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne