Mechanical Properties Metric English Comments
Tensile Stress 1.83 MPa

@Strain 100 %
265 psi

@Strain 100 %
NEU NeuSoft™ 455-60A Ester/ether TPU / SBC blend
Tensile Stress 1.83 MPa

@Strain 41.63 %,
Temperature 100 °C
265 psi

@Strain 41.63 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 3078 Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer with Non-discoloring Stabilizer Hytrel 3078 is a very low modulus grade with nominal hardness of 30D. It contains non-discoloring stabilizer. It can b..
Tensile Stress 1.83 MPa

@Strain 0.0200 %,
Temperature 0.000 °C
265 psi

@Strain 0.0200 %,
Temperature 32.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 54G35EF BK420 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced Toughened PPA High Performance Polyamide Developed for Electrical and Electronics Applications Zytel HTN54G35EF BK420 is a 35% glass reinforced toughened heat stabilized lubrica..
Tensile Stress 1.83 MPa

@Strain 0.0700 %,
Temperature -20.0 °C
265 psi

@Strain 0.0700 %,
Temperature -4.00 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FE8200 NC010 Polyphthalamide (PPA)  (Unverified Data**)
Unreinforced Toughened PPA High Performance Polyamide Zytel HTNFE8200 NC010 is an unreinforced toughened heat stabilized lubricated high performance polyamide resin for injection molding. It is also..
Tensile Stress 1.83 MPa

@Strain 0.0600 %,
Temperature -40.0 °C
265 psi

@Strain 0.0600 %,
Temperature -40.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FE8200 NC010 Polyphthalamide (PPA)  (Unverified Data**)
Unreinforced Toughened PPA High Performance Polyamide Zytel HTNFE8200 NC010 is an unreinforced toughened heat stabilized lubricated high performance polyamide resin for injection molding. It is also..
Tensile Stress 1.83 MPa

@Strain 0.000 %,
Temperature 40.0 °C
265 psi

@Strain 0.000 %,
Temperature 104 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon  (Unverified Data**)
Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood..
Tensile Stress 1.83 MPa

@Strain 41.63 %,
Temperature 100 °C
265 psi

@Strain 41.63 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers