Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 1080 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 7.46 MPa

@Strain 6.00 %,
Temperature 40.0 °C
1080 psi

@Strain 6.00 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 7.46 MPa

@Strain 6.00 %,
Temperature 40.0 °C
1080 psi

@Strain 6.00 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 7.46 MPa

@Strain 0.0500 %,
Temperature 60.0 °C
1080 psi

@Strain 0.0500 %,
Temperature 140 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon  (Unverified Data**)
Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood..
Tensile Stress 7.48 MPa

@Strain 68.02 %,
Temperature 150 °C
1080 psi

@Strain 68.02 %,
Temperature 302 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® RS LC1600 BK385 Nylon 1010  (Unverified Data**)
Zytel® RS LC1600 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced ingredient by weight. It is flexible, toughened, plasticized, UV and heat stabilized and s..
Tensile Stress 7.44 MPa

@Strain 15.0 %,
Temperature 80.0 °C
1080 psi

@Strain 15.0 %,
Temperature 176 °F
ISO 527
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..
Tensile Stress 7.44 MPa

@Strain 60.51 %,
Temperature 120 °C
1080 psi

@Strain 60.51 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc..
Tensile Stress 7.44 MPa

@Strain 21.8 %,
Temperature 100 °C
1080 psi

@Strain 21.8 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me..
Tensile Stress 7.44 MPa

@Strain 21.8 %,
Temperature 100 °C
1080 psi

@Strain 21.8 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET
55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers
Tensile Stress 7.47 MPa

@Strain 0.960 %,
Temperature 90.0 °C
1080 psi

@Strain 0.960 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66  (Unverified Data**)
Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe..
Copyright © lookpolymers.com All Rights Reserved