Mechanical Properties Metric English Comments
Tensile Stress 7.52 MPa

@Strain 300 %
1090 psi

@Strain 300 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ XL-2185 Thermoplastic Polyolefin Elastomer (TPO (POE))
PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o..
Tensile Stress 7.49 MPa

@Strain 0.100 %,
Temperature 80.0 °C
1090 psi

@Strain 0.100 %,
Temperature 176 °F
ISO 11403-1/-2
DuPont Performance Polymers Crastin® LW9330 BK851 PBT  (Unverified Data**)
Crastin® LW9330 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp..
Tensile Stress 7.50 MPa

@Strain 5.00 %,
Temperature 23.0 °C
1090 psi

@Strain 5.00 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® HTR8441 BK316 TPC-ET  (Unverified Data**)
Hytrel® HTR8441 is a 55 nom. Shore D thermoplastic polyester elastomer for blow molding. It provides good mechanical properties at high temperature.Information provided by DuPont Performance Polyme..
Tensile Stress 7.50 MPa

@Strain 100 %
1090 psi

@Strain 100 %
ISO 527-1/-2
DSM Arnitel® EM400-BP TPC-ET
34 Shore D, Injection Molding or Extrusion Grade
Tensile Stress 7.51 MPa

@Strain 0.600 %,
Temperature 100 °C
1090 psi

@Strain 0.600 %,
Temperature 212 °F
ISO 11403-1/-2
DuPont Performance Polymers Delrin® 511P BK402 Acetal Homopolymer
Delrin® 511P is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Information provided ..
Tensile Stress 7.51 MPa

@Strain 16.99 %,
Temperature 90.0 °C
1090 psi

@Strain 16.99 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 7.51 MPa

@Strain 16.99 %,
Temperature 90.0 °C
1090 psi

@Strain 16.99 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 7.51 MPa

@Strain 147.53 %,
Temperature 150 °C
1090 psi

@Strain 147.53 %,
Temperature 302 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 7.49 MPa

@Strain 0.190 %,
Temperature 150 °C
1090 psi

@Strain 0.190 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G35HSRX BK099 Nylon 66  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSRX BK099 a 35% glass reinforced heat stabilized hydrolysis resistant PA66 for injection molding. Developed for applications designed fo..
Tensile Stress 7.51 MPa

@Strain 0.200 %,
Temperature -40.0 °C
1090 psi

@Strain 0.200 %,
Temperature -40.0 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® FR7026V0F NC010 Nylon 66  (Unverified Data**)
Zytel® FR7026V0F NC010 is a flame retardant, heat stabilized, polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by D..
Tensile Stress 7.51 MPa

@Strain 0.150 %,
Temperature 120 °C
1090 psi

@Strain 0.150 %,
Temperature 248 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66  (Unverified Data**)
Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in..
Tensile Stress 7.54 MPa

@Strain 0.0900 %,
Temperature -20.0 °C
1090 psi

@Strain 0.0900 %,
Temperature -4.00 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6  (Unverified Data**)
Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc..
Tensile Stress 7.50 MPa

@Strain 100 %
1090 psi

@Strain 100 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers
Tensile Stress 7.52 MPa

@Strain 20.0 %,
Temperature 100 °C
1090 psi

@Strain 20.0 %,
Temperature 212 °F
ISO 527
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..
Tensile Stress 7.53 MPa

@Strain 17.5 %,
Temperature 100 °C
1090 psi

@Strain 17.5 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc..
Tensile Stress 7.50 MPa

@Strain 5.00 %,
Temperature 23.0 °C
1090 psi

@Strain 5.00 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® G5564 TPC-ET  (Unverified Data**)
Hytrel® G5564 is a 55 nom. Shore D, heat stable, plasticiser free high viscosity resin for extrusion; low temperature impact resistance as well as excellent mechanical properties; good hydrocarbon ..
Tensile Stress 7.52 MPa

@Strain 6.47 %,
Temperature 40.0 °C
1090 psi

@Strain 6.47 %,
Temperature 104 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me..
Tensile Stress 7.54 MPa

@Strain 108.54 %,
Temperature 160 °C
1090 psi

@Strain 108.54 %,
Temperature 320 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me..
Tensile Stress 7.53 MPa

@Strain 130.82 %,
Temperature 120 °C
1090 psi

@Strain 130.82 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 7.54 MPa

@Strain 73.17 %,
Temperature 90.0 °C
1090 psi

@Strain 73.17 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers
Tensile Stress 7.52 MPa

@Strain 6.47 %,
Temperature 40.0 °C
1090 psi

@Strain 6.47 %,
Temperature 104 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET
55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers
Tensile Stress 7.54 MPa

@Strain 108.54 %,
Temperature 160 °C
1090 psi

@Strain 108.54 %,
Temperature 320 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET
55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers
Tensile Stress >= 7.50 MPa

@Strain 300 %
>= 1090 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 382A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech