Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 79.0 MPa @Strain 5.00 %, Temperature 100 °C |
11500 psi @Strain 5.00 %, Temperature 212 °F |
|
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 79.0 MPa @Strain 10.0 %, Temperature 120 °C |
11500 psi @Strain 10.0 %, Temperature 248 °F |
|
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 79.1 MPa @Strain 12.0 %, Temperature 0.000 °C |
11500 psi @Strain 12.0 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 300PE BK602 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 300PE BK602 (formerly DE20577) is a medium-high viscosity acetal homopolymer an enhanced version of Delrin 300CP with very low.. |
|||
Tensile Stress | 79.3 MPa @Strain 18.0 %, Temperature 0.000 °C |
11500 psi @Strain 18.0 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 300PE BK602 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 300PE BK602 (formerly DE20577) is a medium-high viscosity acetal homopolymer an enhanced version of Delrin 300CP with very low.. |
|||
Tensile Stress | 79.5 MPa @Strain 5.20 %, Temperature -20.0 °C |
11500 psi @Strain 5.20 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 527UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized Medium Viscosity Acetal HomopolymerDelrin 527UV NC010 is a medium viscosity acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvem.. |
|||
Tensile Stress | 79.0 MPa @Strain 1.47 %, Temperature 0.000 °C |
11500 psi @Strain 1.47 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FR70M30V0 NC010 Nylon 66
(Unverified Data**) 30% Mineral Reinforced Flame Retardant Polyamide 66 Zytel FR70M30V0 NC010 is a 30% mineral reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performa.. |
|||
Tensile Stress | 79.6 MPa @Strain 1.50 %, Temperature -20.0 °C |
11500 psi @Strain 1.50 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT) 10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 79.5 MPa @Strain 10.5 %, Temperature -20.0 °C |
11500 psi @Strain 10.5 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100 NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Tensile Stress | 79.0 MPa @Strain 4.50 %, Temperature 0.000 °C |
11500 psi @Strain 4.50 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500PE BK602 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE BK602 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
Tensile Stress | 79.6 MPa @Strain 5.00 %, Temperature 0.000 °C |
11500 psi @Strain 5.00 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
Tensile Stress | 79.3 MPa @Strain 1.70 %, Temperature 23.0 °C |
11500 psi @Strain 1.70 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G13L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Polyamide 66Zytel 70G13L NC010 is a 13% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 79.32 MPa @Strain 0.700 %, Temperature 23.0 °C |
11500 psi @Strain 0.700 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN52G35HSL BK083 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin that can be molded in water heated m.. |