Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 1180 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 8.16 MPa

@Strain 300 %,
Temperature 23.0 °C
1180 psi

@Strain 300 %,
Temperature 73.4 °F
Die C Across Flow 2 hr; ASTM D412
PolyOne Versalloy™ HC 9220-90 Thermoplastic Elastomer (TPE)
Versalloy™ HC 9220-90 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr..
Tensile Stress 8.17 MPa

@Strain 0.100 %,
Temperature 23.0 °C
1180 psi

@Strain 0.100 %,
Temperature 73.4 °F
ISO 11403-1/-2
DuPont Performance Polymers Crastin® LW9330 BK851 PBT  (Unverified Data**)
Crastin® LW9330 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp..
Tensile Stress 8.14 MPa

@Strain 100 %
1180 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® C4990 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Stress 8.17 MPa

@Strain 0.240 %,
Temperature -20.0 °C
1180 psi

@Strain 0.240 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 300CP NC010 Acetal (POM)  (Unverified Data**)
Medium-high Viscosity Acetal Homopolymer with Improved ProcessingDelrin 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of proc..
Tensile Stress 8.17 MPa

@Strain 73.69 %,
Temperature 100 °C
1180 psi

@Strain 73.69 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 8.11 MPa

@Strain 34.64 %,
Temperature 100 °C
1180 psi

@Strain 34.64 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers
Tensile Stress 8.17 MPa

@Strain 73.69 %,
Temperature 100 °C
1180 psi

@Strain 73.69 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 8.11 MPa

@Strain 27.16 %,
Temperature 120 °C
1180 psi

@Strain 27.16 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 8.13 MPa

@Strain 87.33 %,
Temperature 120 °C
1180 psi

@Strain 87.33 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 8.12 MPa

@Strain 0.110 %,
Temperature 40.0 °C
1180 psi

@Strain 0.110 %,
Temperature 104 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66  (Unverified Data**)
Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in..
Tensile Stress 8.13 MPa

@Strain 0.110 %,
Temperature 40.0 °C
1180 psi

@Strain 0.110 %,
Temperature 104 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6  (Unverified Data**)
Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc..
Tensile Stress 8.13 MPa

@Strain 0.0400 %,
Temperature 23.0 °C
1180 psi

@Strain 0.0400 %,
Temperature 73.4 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon  (Unverified Data**)
Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood..
Tensile Stress 8.11 MPa

@Strain 120.06 %,
Temperature 100 °C
1180 psi

@Strain 120.06 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G4774 Polyester Elastomer TPC-ET  (Unverified Data**)
47 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4774 is a medium modulus grade with nominal hardness of 47D. It contains discoloring stabilizer. It can be proc..
Tensile Stress 8.17 MPa

@Strain 36.25 %,
Temperature 60.0 °C
1180 psi

@Strain 36.25 %,
Temperature 140 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G4774 Polyester Elastomer TPC-ET  (Unverified Data**)
47 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4774 is a medium modulus grade with nominal hardness of 47D. It contains discoloring stabilizer. It can be proc..
Tensile Stress 8.12 MPa

@Strain 17.37 %,
Temperature 90.0 °C
1180 psi

@Strain 17.37 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc..
Tensile Stress 8.11 MPa

@Strain 126.13 %,
Temperature 100 °C
1180 psi

@Strain 126.13 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8139BK Polyester Elastomer TPC-ET  (Unverified Data**)
44 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR8139BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nomin..
Tensile Stress 8.17 MPa

@Strain 104.16 %,
Temperature 90.0 °C
1180 psi

@Strain 104.16 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 8.12 MPa

@Strain 91.47 %,
Temperature 90.0 °C
1180 psi

@Strain 91.47 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers
Tensile Stress 8.14 MPa

@Strain 99.21 %,
Temperature 150 °C
1180 psi

@Strain 99.21 %,
Temperature 302 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Copyright © lookpolymers.com All Rights Reserved