Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 8.62 MPa @Strain 300 % |
1250 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® A9875H TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Stress | 8.62 MPa @Strain 0.320 %, Temperature 23.0 °C |
1250 psi @Strain 0.320 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S620F20 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S620F20 NC010 is an unreinforced nucleated lubricated medium viscosity polybutylene terephthalate resin for fast injection molding.In.. |
|||
Tensile Stress | 8.62 MPa @Strain 204.54 %, Temperature 100 °C |
1250 psi @Strain 204.54 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.65 MPa @Strain 47.36 %, Temperature 90.0 °C |
1250 psi @Strain 47.36 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.61 MPa @Strain 170.01 %, Temperature 120 °C |
1250 psi @Strain 170.01 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.64 MPa @Strain 85.36 %, Temperature 100 °C |
1250 psi @Strain 85.36 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.65 MPa @Strain 47.36 %, Temperature 90.0 °C |
1250 psi @Strain 47.36 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.61 MPa @Strain 74.05 %, Temperature 120 °C |
1250 psi @Strain 74.05 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.64 MPa @Strain 30.0 %, Temperature 80.0 °C |
1250 psi @Strain 30.0 %, Temperature 176 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.64 MPa @Strain 5.00 %, Temperature 0.000 °C |
1250 psi @Strain 5.00 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.62 MPa @Strain 2.15 %, Temperature 150 °C |
1250 psi @Strain 2.15 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Unreinforced Polyamide 6 Zytel 7335F NC010 is a nucleated lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.60 MPa @Strain 2.40 %, Temperature 150 °C |
1250 psi @Strain 2.40 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® E51HSB NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized High Viscosity Polyamide 66 Zytel E51HSB NC010 is a high molecular weight heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by .. |
|||
Tensile Stress | 8.59 MPa @Strain 0.200 %, Temperature 150 °C |
1250 psi @Strain 0.200 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G20NH BK337 Polyphthalamide (PPA) Zytel® HTNFR52G20NH BK337 is a 20% glass reinforced, flame retardant, lubricated high performance polyamide resin. It is also a PPA resin and it uses a non-halogenated flame retardant.Information p.. |
|||
Tensile Stress | 8.65 MPa @Strain 0.100 %, Temperature 40.0 °C |
1250 psi @Strain 0.100 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FR52G20NH NC010 Polyphthalamide (PPA)
(Unverified Data**) 20% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G20NH NC010 is a 20% glass reinforced flame retardant lubricated high performance polyamide resin. It.. |
|||
Tensile Stress | 8.61 MPa @Strain 37.5 %, Temperature 100 °C |
1250 psi @Strain 37.5 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc.. |
|||
Tensile Stress | 8.63 MPa @Strain 66.51 %, Temperature 120 °C |
1250 psi @Strain 66.51 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me.. |
|||
Tensile Stress | 8.64 MPa @Strain 34.94 %, Temperature 100 °C |
1250 psi @Strain 34.94 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me.. |
|||
Tensile Stress | 8.62 MPa @Strain 44.89 %, Temperature 120 °C |
1250 psi @Strain 44.89 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.63 MPa @Strain 66.51 %, Temperature 120 °C |
1250 psi @Strain 66.51 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET 55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.64 MPa @Strain 34.94 %, Temperature 100 °C |
1250 psi @Strain 34.94 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET 55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.62 MPa @Strain 1.25 %, Temperature 150 °C |
1250 psi @Strain 1.25 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 73M40 NC010 Nylon 6
(Unverified Data**) 40% Mineral Reinforced Polyamide 6 Minlon 73M40 NC010 is a 40% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro.. |
|||
Tensile Stress | 8.62 MPa @Strain 100 % |
1250 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ P45D-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P45D-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 8.62 MPa @Strain 100 % |
1250 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ P45D-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P45D-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |