Polymer Property : Tensile Stress = 1260 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 8.69 MPa

@Strain 300 %
1260 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® F02-074B-8 TPE, Halogen Free Extrusion Grade
Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to..
Tensile Stress 8.70 MPa

@Strain 0.900 %,
Temperature 90.0 °C
1260 psi

@Strain 0.900 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500AF Acetal (POM)  (Unverified Data**)
20% Teflon® Fiber Filled Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AF is a medium viscosity acetal homopolymer resin containing 20% Teflon PTFE fibers. It is desi..
Tensile Stress 8.67 MPa

@Strain 7.52 %,
Temperature 40.0 °C
1260 psi

@Strain 7.52 %,
Temperature 104 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 8.67 MPa

@Strain 7.52 %,
Temperature 40.0 °C
1260 psi

@Strain 7.52 %,
Temperature 104 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 8.70 MPa

@Strain 65.06 %,
Temperature 90.0 °C
1260 psi

@Strain 65.06 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT  (Unverified Data**)
Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 8.69 MPa

@Strain 0.100 %,
Temperature 60.0 °C
1260 psi

@Strain 0.100 %,
Temperature 140 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® HTN FR52G20NH BK337 Polyphthalamide (PPA)
Zytel® HTNFR52G20NH BK337 is a 20% glass reinforced, flame retardant, lubricated high performance polyamide resin. It is also a PPA resin and it uses a non-halogenated flame retardant.Information p..
Tensile Stress 8.71 MPa

@Strain 0.230 %,
Temperature 150 °C
1260 psi

@Strain 0.230 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® PLS 93G35DH1 BK549 Nylon 6  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 6 Information provided by DuPont Performance Polymers
Tensile Stress 8.71 MPa

@Strain 0.100 %,
Temperature 23.0 °C
1260 psi

@Strain 0.100 %,
Temperature 73.4 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66  (Unverified Data**)
Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in..
Tensile Stress 8.71 MPa

@Strain 0.230 %,
Temperature 150 °C
1260 psi

@Strain 0.230 %,
Temperature 302 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6  (Unverified Data**)
Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc..
Tensile Stress 8.68 MPa

@Strain 0.0500 %,
Temperature 0.000 °C
1260 psi

@Strain 0.0500 %,
Temperature 32.0 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon  (Unverified Data**)
Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood..
Tensile Stress 8.70 MPa

@Strain 21.27 %,
Temperature 150 °C
1260 psi

@Strain 21.27 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC1610 BK387 Nylon 1010  (Unverified Data**)
Plasticized Toughened Renewably Sourced Polyamide 1010 Developed for Extrusion Information provided by DuPont Performance Polymers
Tensile Stress 8.67 MPa

@Strain 40.0 %,
Temperature 100 °C
1260 psi

@Strain 40.0 %,
Temperature 212 °F
ISO 527
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..
Tensile Stress 8.67 MPa

@Strain 0.360 %,
Temperature -40.0 °C
1260 psi

@Strain 0.360 %,
Temperature -40.0 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET  (Unverified Data**)
65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers
Tensile Stress 8.66 MPa

@Strain 9.79 %,
Temperature -20.0 °C
1260 psi

@Strain 9.79 %,
Temperature -4.00 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 8.69 MPa

@Strain 175.85 %,
Temperature 120 °C
1260 psi

@Strain 175.85 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 8.69 MPa

@Strain 114.16 %,
Temperature 150 °C
1260 psi

@Strain 114.16 %,
Temperature 302 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 8.66 MPa

@Strain 0.200 %,
Temperature 150 °C
1260 psi

@Strain 0.200 %,
Temperature 302 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66  (Unverified Data**)
Zytel® 80G43HS1L BK104 is a 43% glass fiber reinforced, heat stabilized, black polyamide 66 resin with superior impact resistance.Information provided by DuPont Performance Polymers