Polymer Property : Tensile Stress = 1330 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 9.20 MPa

@Strain 300 %,
Thickness 2.00 mm
1330 psi

@Strain 300 %,
Thickness 0.0787 in
Type 1, 200 mm/min; Flow; DIN 53504
PolyOne OnFlex™ BIO 5370A-E0004 Thermoplastic Elastomer (TPE)
OnFlex™-Bio 5300 series thermoplastic elastomer compounds are soft thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% of renewable materi..
Tensile Stress 9.17 MPa

@Strain 300 %
1330 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® C4995 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Stress 9.16 MPa

@Strain 100 %,
Temperature 21.0 °C
1330 psi

@Strain 100 %,
Temperature 69.8 °F
Die C Flow 2 hr; ASTM D412
PolyOne Versalloy™ HC 9220-90 Thermoplastic Elastomer (TPE)
Versalloy™ HC 9220-90 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr..
Tensile Stress 9.17 MPa

@Strain 300 %
1330 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P2885 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 9.18 MPa

@Strain 6.32 %,
Temperature 90.0 °C
1330 psi

@Strain 6.32 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)  (Unverified Data**)&
Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo..
Tensile Stress 9.14 MPa

@Strain 0.550 %,
Temperature 150 °C
1330 psi

@Strain 0.550 %,
Temperature 302 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5315HF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5315HF is a 15% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen..
Tensile Stress 9.14 MPa

@Strain 221.82 %,
Temperature 100 °C
1330 psi

@Strain 221.82 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET  (Unverified Data**)
45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 9.14 MPa

@Strain 87.12 %,
Temperature 90.0 °C
1330 psi

@Strain 87.12 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 9.17 MPa

@Strain 133.96 %,
Temperature 100 °C
1330 psi

@Strain 133.96 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 9.18 MPa

@Strain 119.65 %,
Temperature 100 °C
1330 psi

@Strain 119.65 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers
Tensile Stress 9.19 MPa

@Strain 70.25 %,
Temperature 90.0 °C
1330 psi

@Strain 70.25 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers
Tensile Stress 9.14 MPa

@Strain 87.12 %,
Temperature 90.0 °C
1330 psi

@Strain 87.12 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 9.17 MPa

@Strain 133.96 %,
Temperature 100 °C
1330 psi

@Strain 133.96 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 9.15 MPa

@Strain 120.1 %,
Temperature 120 °C
1330 psi

@Strain 120.1 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 9.16 MPa

@Strain 17.23 %,
Temperature 100 °C
1330 psi

@Strain 17.23 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 9.20 MPa

@Strain 47.92 %,
Temperature 100 °C
1330 psi

@Strain 47.92 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 9.20 MPa

@Strain 45.0 %,
Temperature 80.0 °C
1330 psi

@Strain 45.0 %,
Temperature 176 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT  (Unverified Data**)
Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 9.17 MPa

@Strain 0.200 %,
Temperature 0.000 °C
1330 psi

@Strain 0.200 %,
Temperature 32.0 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® FR7026V0F NC010 Nylon 66  (Unverified Data**)
Zytel® FR7026V0F NC010 is a flame retardant, heat stabilized, polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by D..
Tensile Stress 9.15 MPa

@Strain 0.100 %,
Temperature 23.0 °C
1330 psi

@Strain 0.100 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FR52G20NH NC010 Polyphthalamide (PPA)  (Unverified Data**)
20% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G20NH NC010 is a 20% glass reinforced flame retardant lubricated high performance polyamide resin. It..
Tensile Stress 9.16 MPa

@Strain 0.180 %,
Temperature 90.0 °C
1330 psi

@Strain 0.180 %,
Temperature 194 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6  (Unverified Data**)
Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc..
Tensile Stress 9.18 MPa

@Strain 0.390 %,
Temperature -40.0 °C
1330 psi

@Strain 0.390 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC1010 NC010 Nylon 1010  (Unverified Data**)
Unreinforced Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight. ..
Tensile Stress 9.15 MPa

@Strain 24.0 %,
Temperature 90.0 °C
1330 psi

@Strain 24.0 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc..
Tensile Stress 9.20 MPa

@Strain 195.71 %,
Temperature 120 °C
1330 psi

@Strain 195.71 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 9.20 MPa

@Strain 128.33 %,
Temperature 150 °C
1330 psi

@Strain 128.33 %,
Temperature 302 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 9.18 MPa

@Strain 0.770 %,
Temperature 23.0 °C
1330 psi

@Strain 0.770 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66  (Unverified Data**)
Toughened Heat Stabilized Polyamide 66 Zytel 444AHS is a toughened heat stabilized black polyamide 66 resin for injection molding. It is a high flow processing friendly material.Information provided..