Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 21.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 21.0 MPa

@Strain 8.14 %,
Temperature 90.0 °C
3050 psi

@Strain 8.14 %,
Temperature 194 °F
ISO 527
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers
Tensile Stress 21.0 MPa

@Strain 3.00 %,
Temperature 160 °C
3050 psi

@Strain 3.00 %,
Temperature 320 °F
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY
Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th..
Tensile Stress 21.0 MPa

@Strain 6.00 %,
Temperature 200 °C
3050 psi

@Strain 6.00 %,
Temperature 392 °F
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY
Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th..
Tensile Stress 21.0 MPa

@Strain 20.0 %,
Temperature 150 °C
3050 psi

@Strain 20.0 %,
Temperature 302 °F
Solvay TECHNYL® A 205F PA66, DRY
Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities..
Tensile Stress 21.0 MPa

@Strain 50.0 %
3050 psi

@Strain 50.0 %
dry; ISO 527-1/-2
EMS-Grivory Grivory® ELX 40 HNZ TPA
Product description: Grilon ELX 40 H NZ is a high viscosity, heat stabilized, impact modified, thermoplastic PA6 elastomer for extrusion blow moulding applications. Grilon ELX 40 H NZ has the follow..
Tensile Stress 21.0 MPa

@Strain 4.40 %,
Temperature 90.0 °C
3050 psi

@Strain 4.40 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)  (Unverified Data**)
Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri..
Tensile Stress 21.0 MPa

@Strain 0.500 %,
Temperature -40.0 °C
3050 psi

@Strain 0.500 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 511DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s..
Tensile Stress 21.0 MPa

@Strain 0.500 %,
Temperature -40.0 °C
3050 psi

@Strain 0.500 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo..
Tensile Stress 21.0 MPa

@Strain 5.34 %,
Temperature 40.0 °C
3050 psi

@Strain 5.34 %,
Temperature 104 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® LC6200 BK385 Nylon 612  (Unverified Data**)
Toughened Polyamide 612 Developed for ExtrusionInformation provided by DuPont Performance Polymers
Tensile Stress 21.0 MPa

@Strain 100 %
3050 psi

@Strain 100 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me..
Tensile Stress 21.0 MPa

@Strain 100 %
3050 psi

@Strain 100 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET
55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers
Tensile Stress 21.0 MPa

@Strain 300 %
3050 psi

@Strain 300 %
ASTM D412
Alliance Polymers Zythane™ 4045D Thermoplastic Polyurethane Elastomer
Zythane™ 4045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Stress >= 21.0 MPa

@Strain 300 %
>= 3050 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 395A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech
Tensile Stress 21.0 MPa

@Strain 0.400 %,
Temperature 23.0 °C
3050 psi

@Strain 0.400 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 12T NC010 Nylon 66  (Unverified Data**)
36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T NC010 is a 36% mineral reinforced toughened heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performan..