Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 15.0 MPa @Strain 10.0 %, Temperature 23.0 °C |
2180 psi @Strain 10.0 %, Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® 6359FG NC010 TPC-ET
(Unverified Data**) Hytrel® 6359FG is a medium modulus Hytrel® grade with nominal durometer hardness of 63D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing t.. |
|||
Tensile Stress | 15.0 MPa @Strain 10.0 %, Temperature 23.0 °C |
2180 psi @Strain 10.0 %, Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® HTR8730 BK320 TPC-ET
(Unverified Data**) Hytrel® HTR8730 BK320 is a high viscosity thermoplastic polyester elastomer designed for blow molding. It has excellent mechanical properties at elevated temperatures and very good resistance to mo.. |
|||
Tensile Stress | 15.0 MPa @Strain 1.00 %, Temperature 80.0 °C |
2180 psi @Strain 1.00 %, Temperature 176 °F |
|
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th.. |
|||
Tensile Stress | 15.0 MPa @Strain 6.00 %, Temperature 230 °C |
2180 psi @Strain 6.00 %, Temperature 446 °F |
|
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th.. |
|||
Tensile Stress | 15.0 MPa @Strain 20.0 %, Temperature 135 °C |
2180 psi @Strain 20.0 %, Temperature 275 °F |
|
Solvay TECHNYL® eXten D 437P PA6.10 Description: TECHNYL® eXten D 437P is a high viscosity, unfilled, plasticized, UV and heat stabilized PA6.10 for extrusion applications. Technyl® eXten D 437P is a partially biosourced materia.. |
|||
Tensile Stress | 15.0 MPa @Strain 160 %, Temperature 150 °C |
2180 psi @Strain 160 %, Temperature 302 °F |
|
Solvay TECHNYL® eXten D 437P PA6.10 Description: TECHNYL® eXten D 437P is a high viscosity, unfilled, plasticized, UV and heat stabilized PA6.10 for extrusion applications. Technyl® eXten D 437P is a partially biosourced materia.. |
|||
Tensile Stress | 15.0 MPa @Strain 2.50 %, Temperature 23.0 °C |
2180 psi @Strain 2.50 %, Temperature 73.4 °F |
|
Solvay TECHNYL® A 205F PA66, Conditioned Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Tensile Stress | 15.0 MPa @Strain 5.00 %, Temperature 80.0 °C |
2180 psi @Strain 5.00 %, Temperature 176 °F |
|
Solvay TECHNYL® A 205F PA66, Conditioned Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Tensile Stress | 15.0 MPa @Strain 10.0 %, Temperature 150 °C |
2180 psi @Strain 10.0 %, Temperature 302 °F |
|
Solvay TECHNYL® A 205F PA66, DRY Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Tensile Stress | 15.0 MPa @Strain 0.130 %, Time 3600 sec |
2180 psi @Strain 0.130 %, Time 1.00 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7.. |
|||
Tensile Stress | 15.0 MPa @Strain 0.150 %, Time 36000 sec |
2180 psi @Strain 0.150 %, Time 10.0 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7.. |
|||
Tensile Stress | 15.0 MPa @Strain 0.170 %, Time 360000 sec |
2180 psi @Strain 0.170 %, Time 100 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7.. |
|||
Tensile Stress | 15.0 MPa @Strain 100 % |
2180 psi @Strain 100 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 15.0 MPa @Strain 10.0 % |
2180 psi @Strain 10.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 15.0 MPa @Strain 10.0 % |
2180 psi @Strain 10.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 15.0 MPa @Strain 0.250 %, Temperature 0.000 °C |
2180 psi @Strain 0.250 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT) 10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 15.0 MPa @Strain 100 % |
2180 psi @Strain 100 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR237BG BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR237BG is designed for blow molding or processing techniques requiring high viscosity. It has nominal dur.. |
|||
Tensile Stress | 15.0 MPa @Strain 10.0 % |
2180 psi @Strain 10.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR8730 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Viscosity Polyester Elastomer with Excellent Mechanical Properties at Elevated Temperatures Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 15.0 MPa @Strain 300 % |
2180 psi @Strain 300 % |
ASTM D412 |
Alliance Polymers Zythane™ 4085A Thermoplastic Polyurethane Elastomer Zythane™ 4085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 15.0 MPa @Strain 300 % |
2180 psi @Strain 300 % |
ASTM D412 |
Alliance Polymers Zythane™ 6090A Thermoplastic Polyurethane Elastomer Zythane™ 6090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 15.0 MPa @Strain 2.00 %, Time 3.60e+7 sec |
2180 psi @Strain 2.00 %, Time 10000 hour |
ISO 899-1 |
BASF Ultraform N 2320 003 UNC Q600 POM Ultraform N 2320 003 UNC Q600 is a rapidly solidifying grade of POM for injection molding. Contains a mold release agent. |
|||
Tensile Stress | 15.0 MPa @Strain 200 % |
2180 psi @Strain 200 % |
|
AorTech Biomaterials Elast-Eon™ E2-945 Biomedical Polyurethane Pellets Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation. |
|||
Tensile Stress | 15.0 MPa @Strain 200 % |
2180 psi @Strain 200 % |
|
AorTech Biomaterials Elast-Eon™ E2-945 Biomedical Polyurethane Pellets Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation. |
|||
Tensile Stress | >= 15.0 MPa @Strain 300 % |
>= 2180 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 290A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Tensile Stress | >= 15.0 MPa @Strain 100 % |
>= 2180 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 495A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tensile Stress | >= 15.0 MPa @Strain 100 % |
>= 2180 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 364D Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Tensile Stress | >= 15.0 MPa @Strain 100 % |
>= 2180 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 598A Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |
|||
Tensile Stress | 15.0 MPa @Strain 300 % |
2180 psi @Strain 300 % |
ASTM D412 |
Alliance Polymers Zythane™ 7090A Thermoplastic Polyurethane Elastomer Zythane™ 7090A is a polyether-based TPU specifically formulated for extrusion molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good hydroly.. |
|||
Tensile Stress | 15.0 MPa @Strain 15.0 %, Time 3.60e+6 sec |
2180 psi @Strain 15.0 %, Time 1000 hour |
100°C; ISO 527 |
BASF Ultradur B 4520 PBT Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade. |