Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 1.83 MPa @Strain 100 % |
265 psi @Strain 100 % |
|
NEU NeuSoft™ 455-60A Ester/ether TPU / SBC blend |
|||
Tensile Stress | 1.83 MPa @Strain 41.63 %, Temperature 100 °C |
265 psi @Strain 41.63 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 3078 Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D High Performance Polyester Elastomer with Non-discoloring Stabilizer Hytrel 3078 is a very low modulus grade with nominal hardness of 30D. It contains non-discoloring stabilizer. It can b.. |
|||
Tensile Stress | 1.83 MPa @Strain 0.0200 %, Temperature 0.000 °C |
265 psi @Strain 0.0200 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 54G35EF BK420 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced Toughened PPA High Performance Polyamide Developed for Electrical and Electronics Applications Zytel HTN54G35EF BK420 is a 35% glass reinforced toughened heat stabilized lubrica.. |
|||
Tensile Stress | 1.83 MPa @Strain 0.0700 %, Temperature -20.0 °C |
265 psi @Strain 0.0700 %, Temperature -4.00 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FE8200 NC010 Polyphthalamide (PPA)
(Unverified Data**) Unreinforced Toughened PPA High Performance Polyamide Zytel HTNFE8200 NC010 is an unreinforced toughened heat stabilized lubricated high performance polyamide resin for injection molding. It is also.. |
|||
Tensile Stress | 1.83 MPa @Strain 0.0600 %, Temperature -40.0 °C |
265 psi @Strain 0.0600 %, Temperature -40.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FE8200 NC010 Polyphthalamide (PPA)
(Unverified Data**) Unreinforced Toughened PPA High Performance Polyamide Zytel HTNFE8200 NC010 is an unreinforced toughened heat stabilized lubricated high performance polyamide resin for injection molding. It is also.. |
|||
Tensile Stress | 1.83 MPa @Strain 0.000 %, Temperature 40.0 °C |
265 psi @Strain 0.000 %, Temperature 104 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon
(Unverified Data**) Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood.. |
|||
Tensile Stress | 1.83 MPa @Strain 41.63 %, Temperature 100 °C |
265 psi @Strain 41.63 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |