Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.55 MPa @Strain 100 %, Temperature 23.0 °C |
370 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versollan™ OM 1262NX-1 Thermoplastic Elastomer (TPE) Versollan™ OM 1262NX-1 is a performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS and PC/ABS substrates. - Excellent Grip with Matte, Rubbery Finish - Proven Track R.. |
|||
Tensile Stress | 2.55 MPa @Strain 100 %, Temperature 23.0 °C |
370 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versollan™ OM 1262NX-9 Thermoplastic Elastomer (TPE) Versollan™ OM 1262NX-9 is a performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS, PC/ABS and copolyester substrates. - Excellent Grip with Matte, Rubbery Finish - P.. |
|||
Tensile Stress | 2.55 MPa @Strain 100 % |
370 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® D6760 TPE, Extruded Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from.. |
|||
Tensile Stress | 2.55 MPa @Strain 300 %, Temperature 23.0 °C |
370 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G2711-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2711-1000-00 is an easy process compound designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - O.. |
|||
Tensile Stress | 2.55 MPa @Strain 100 % |
370 psi @Strain 100 % |
ASTM D412 |
Teknor Apex Telcar® TL-1221A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Stress | 2.55 MPa @Strain 93.75 %, Temperature 90.0 °C |
370 psi @Strain 93.75 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 3078 Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D High Performance Polyester Elastomer with Non-discoloring Stabilizer Hytrel 3078 is a very low modulus grade with nominal hardness of 30D. It contains non-discoloring stabilizer. It can b.. |
|||
Tensile Stress | 2.55 MPa @Strain 26.74 %, Temperature 60.0 °C |
370 psi @Strain 26.74 %, Temperature 140 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 3078 Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D High Performance Polyester Elastomer with Non-discoloring Stabilizer Hytrel 3078 is a very low modulus grade with nominal hardness of 30D. It contains non-discoloring stabilizer. It can b.. |
|||
Tensile Stress | 2.55 MPa @Strain 93.75 %, Temperature 90.0 °C |
370 psi @Strain 93.75 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.55 MPa @Strain 26.74 %, Temperature 60.0 °C |
370 psi @Strain 26.74 %, Temperature 140 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |