Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 5.52 MPa @Strain 300 % |
800 psi @Strain 300 % |
|
NEU NeuSoft™ 455-60A Ester/ether TPU / SBC blend |
|||
Tensile Stress | 5.52 MPa @Strain 100 % |
801 psi @Strain 100 % |
510 mm/min; ASTM D412A |
PolyOne Elastamax™ XL 0135-33 Styrene Butadiene Block Copolymer (SBC) A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco.. |
|||
Tensile Stress | 5.52 MPa @Strain 100 % |
801 psi @Strain 100 % |
510 mm/min; ASTM D412A |
PolyOne Elastamax™ XL-2085 Thermoplastic Polyolefin Elastomer (TPO (POE)) PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o.. |
|||
Tensile Stress | 5.52 MPa @Strain 0.0400 %, Temperature 0.000 °C |
801 psi @Strain 0.0400 %, Temperature 32.0 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66
(Unverified Data**) Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in.. |
|||
Tensile Stress | 5.52 MPa @Strain 0.0700 %, Temperature 60.0 °C |
801 psi @Strain 0.0700 %, Temperature 140 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6
(Unverified Data**) Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc.. |