Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 5.60 MPa @Strain 0.400 %, Temperature 90.0 °C |
812 psi @Strain 0.400 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 300PE BK602 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 300PE BK602 (formerly DE20577) is a medium-high viscosity acetal homopolymer an enhanced version of Delrin 300CP with very low.. |
|||
Tensile Stress | 5.60 MPa @Strain 100 % |
812 psi @Strain 100 % |
ASTM D412 |
ExxonMobil Vistamaxx™ 3980FL Propylene-based Elastomer - High Purity, Low Gel Product Description: Vistamaxx 3980FL propylene-based elastomer is an olefinic elastomer primarily composed of isostatic propylene repeat units with random ethylene distribution. It is produced us.. |
|||
Tensile Stress | 5.60 MPa @Strain 0.400 %, Temperature 90.0 °C |
812 psi @Strain 0.400 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
Tensile Stress | 5.60 MPa @Strain 17.63 %, Temperature 90.0 °C |
812 psi @Strain 17.63 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4774 Polyester Elastomer TPC-ET
(Unverified Data**) 47 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4774 is a medium modulus grade with nominal hardness of 47D. It contains discoloring stabilizer. It can be proc.. |
|||
Tensile Stress | 5.60 MPa @Strain 84.36 %, Temperature 120 °C |
812 psi @Strain 84.36 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8139BK Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR8139BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nomin.. |
|||
Tensile Stress | 5.60 MPa @Strain 159.43 %, Temperature 180 °C |
812 psi @Strain 159.43 %, Temperature 356 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET
(Unverified Data**) 65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers |