Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 9.60 MPa @Strain 0.54861 %, Temperature 120 °C |
1390 psi @Strain 0.54861 %, Temperature 248 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 510GR NC000 Acetal Homopolymer
(Unverified Data**) Delrin® 510GR is a 10% glass reinforced acetal homopolymer for injection molding. It has high strength, stiffness, and high deflection temperature and excellent creep resistance.Information provide.. |
|||
Tensile Stress | 9.60 MPa @Strain 196.16 %, Temperature 120 °C |
1390 psi @Strain 196.16 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 9.60 MPa @Strain 196.16 %, Temperature 120 °C |
1390 psi @Strain 196.16 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 9.60 MPa @Strain 13.16 %, Temperature 90.0 °C |
1390 psi @Strain 13.16 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC4601 NC010 Nylon
(Unverified Data**) Plasticized Toughened Renewably Sourced Polyamide Developed for Extrusion Zytel RS LC4601 NC010 is a flexible toughened and plasticized polyamide resin intended for extrusion applications.Informatio.. |
|||
Tensile Stress | 9.60 MPa @Strain 10.0 %, Temperature 23.0 °C |
1390 psi @Strain 10.0 %, Temperature 73.4 °F |
ASTM D638 |
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET
(Unverified Data**) Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various.. |
|||
Tensile Stress | 9.60 MPa @Strain 1.23 %, Time 360000 sec |
1390 psi @Strain 1.23 %, Time 100 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 73M30 NC010 Nylon 6
(Unverified Data**) 30% Mineral Reinforced Polyamide 6 Minlon 73M30 NC010 is a 30% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro.. |
|||
Tensile Stress | 9.60 MPa @Strain 0.874 %, Time 3600 sec |
1390 psi @Strain 0.874 %, Time 1.00 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 73M30 NC010 Nylon 6
(Unverified Data**) 30% Mineral Reinforced Polyamide 6 Minlon 73M30 NC010 is a 30% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro.. |
|||
Tensile Stress | 9.60 MPa @Strain 1.51 %, Time 3.60e+7 sec |
1390 psi @Strain 1.51 %, Time 10000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 73M30 NC010 Nylon 6
(Unverified Data**) 30% Mineral Reinforced Polyamide 6 Minlon 73M30 NC010 is a 30% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro.. |
|||
Tensile Stress | 9.60 MPa @Strain 1.05 %, Time 36000 sec |
1390 psi @Strain 1.05 %, Time 10.0 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 73M30 NC010 Nylon 6
(Unverified Data**) 30% Mineral Reinforced Polyamide 6 Minlon 73M30 NC010 is a 30% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro.. |
|||
Tensile Stress | 9.60 MPa @Strain 1.37 %, Time 3.60e+6 sec |
1390 psi @Strain 1.37 %, Time 1000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 73M30 NC010 Nylon 6
(Unverified Data**) 30% Mineral Reinforced Polyamide 6 Minlon 73M30 NC010 is a 30% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro.. |
|||
Tensile Stress | 9.60 MPa @Strain 0.902 %, Time 3600 sec |
1390 psi @Strain 0.902 %, Time 1.00 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 9.60 MPa @Strain 1.47 %, Time 360000 sec |
1390 psi @Strain 1.47 %, Time 100 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 9.60 MPa @Strain 1.15 %, Time 36000 sec |
1390 psi @Strain 1.15 %, Time 10.0 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 9.60 MPa @Strain 2.36 %, Time 3.60e+7 sec |
1390 psi @Strain 2.36 %, Time 10000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 9.60 MPa @Strain 1.89 %, Time 3.60e+6 sec |
1390 psi @Strain 1.89 %, Time 1000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |