Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Strength = 10200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 70.0 - 100 MPa
10200 - 14500 psi
Compression; ISO 178
Raschig Group MELOPLAS® 150 MF
Wood flour-reinforced MF molding compound in dark colors. High surface hardness, high mechanical strength, good electrical properties. Self-extinguishing (V-O/1,6 according to UL 94), UL-listed. Fr..
Flexural Strength 70.3 MPa
10200 psi
ASTM D790
Ravago Manufacturing Americas Hysun™ 678UV ASA
Available in North America Additive: UV Stabilizer Features: Good Impact Resistance and High Heat ResistanceRoHS CompliantForm: PelletsInformation provided by Ravago
Flexural Strength 70.0 MPa
10200 psi
Lehmann & Voss LUVOCOM® 1-7968 Polyamide 66, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Dynamic stressed parts.Isotrop..
Flexural Strength 70.0 MPa
10200 psi
Lehmann & Voss LUVOCOM® 80-0837 Polyacetal-copolymer, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Flexural Strength 70.0 MPa
10200 psi
Lehmann & Voss LUVOCOM® 80-7014 Polyacetal-copolymer, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Flexural Strength 70.0 MPa
10200 psi
2 mm/min; ISO 178
Lucite International Perspexâ„¢ XT IM60 Acrylic Impact Modified Extruded Sheet
PERSPEX extruded sheet has a lower molecular weight making it easy to vacuum form and the extrusion process gives excellent thickness tolerance and is economical for long production runs.Information..
Flexural Strength 70.0 MPa
10200 psi
Lushan PP+GF30% Maleic Anhydride Grafted Polypropylene
Malic anhydride grafted polypropylene (PP-a-MAH) Lushan series is evaluated as compatiblizer/coupling agent which is used to fill or reinforced polypropylene. As the coupling agent, PP-g-MAH can sig..
Flexural Strength 70.0 MPa
10200 psi
Lehmann & Voss LUVOCOM® 1850-7557 PBT, with aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour, self-lubricating, for highest tribologic needs.Low warpag..
Flexural Strength 70.0 MPa
10200 psi
2mm/min; ASTM D790
Kingfa NH-627 Flame Retardant ABS
Features:UL 94 V-2 @ 1.6mmHalogen-free flame retardantHigh flowApplications:OA deviceDigital cameraVidiconInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Flexural Strength 70.0 MPa
10200 psi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP DL0049EF PC (Asia Pacific)
LNP* Lubricomp* DL0049EF is a compound based on Polycarbonate resin containing PTFE, Flame Retardant. Added features of this material include: Internally Lubricated.
Flexural Strength 70.0 MPa
10200 psi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer
LNP* LUBRICOMP* KG002 is a compound based on Acetal Copolymer resin containing 10% Graphite. Added feature of this material is: Wear Resistant.
Flexural Strength 70.0 MPa
10200 psi
DIN 54352
Schwartz Technical Plastics LAMIGAMID® 320 Cast Polyamide 6, Conditioned
Application: heavy-duty wheelsInformation provided by Schwartz Technical Plastics GmbH
Flexural Strength 70.0 MPa
10200 psi
ISO 178
Styrolution Novodur® 4115 ABS
Novodur Ultra 4115 is a PC modified high heat injection molding grade. It provides good heat resistance combined with high impact strength.Information provided by Styrolution
Flexural Strength 70.0 MPa
10200 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP KZ004 Acetal Copolymer (Asia Pacific)
LNP* THERMOCOMP* KZ004 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass.
Flexural Strength 70.0 MPa
10200 psi
ISO 178
Styrolution PS 153F GPPS
Styrolution PS 153F is general purpose polystyrene with high heat resistance and good flow properties. Styrolution PS 153F is free of internal lubricants, e.g. zinc stearate.Free of internal lubrica..
Flexural Strength 70.6 MPa
10200 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® QU-0191S ABS, Unreinforced Extrusion Grade
Information provided by Samsung Cheil Industries.
Flexural Strength 70.0 MPa
10200 psi
3 points and 2 mm/min; ISO 178
Styron Magnumâ„¢ 3513 Acrylonitrile Butadiene Styrene (ABS)
MAGNUMâ„¢ 3513 is a grade which combines high impact with good flowability. It is suitable for injection molding and extrusion applications.Information provided by DowThis product line was spun ..
Flexural Strength 70.0 MPa
10200 psi
ASTM D790
Sumitomo Bakelite North America RX® 448 Cellulose Reinforced Phenolic Novolac
RX448 is a cellulose fiber reinforced phenolic novolac molding compound. This material is recommended for large parts requiring moderate toughness. It is designed to meet the requirements of ASTM D..
Flexural Strength 70.0 MPa
10200 psi
ISO 178-93
Wellman Wellpet® PR118-N2 Unfilled Polyester PET
Description: Unfilled Polyester PETInformation provided by Wellman.
Flexural Strength 70.0 MPa
10200 psi
DIN EN ISO 178
Wolf Kunststoff ZEDEX® ZX-530KF15 A5M Polymer Alloy
Main Characteristics: High elongation; High impact strength; Stress resistantApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInformation provided by Zed..
Flexural Strength 70.0 MPa
10200 psi
ISO 178
Polyram RamShine PAS702 ASA, UV Stabilized
UV stabilized, general purpose, injection molding ASA.Information provided by Polyram.
Flexural Strength 70.0 MPa
10200 psi
ASTM-D790
Polyram RamTal PM1419 Acetal, PTFE Filled
Polyacetal filled with PTFE for sliding parts, low friction and improved wear resistance in molded parts.Information provided by Polyram Ram On Ind.
Flexural Strength 70.0 MPa
10200 psi
ASTM D790
Eastman Eastman 1223 Copolyester
Applications:Blown filmCredit cardsDebit cardsDeodorant packagingElectronic packagingFabricated boxesFlexible packagingFood packagingFurniture/Furniture trimGaming cardsGift cardsIdentification card..
Flexural Strength 70.0 MPa
10200 psi
ISO 178
Denka MALECCA K-510 ABS
A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de..
Flexural Strength 70.0 MPa
10200 psi
ISO 178
Eurostar Staramide R1000EI2 PA66, Impact Modified, Injection Molded
Staramide R1000EI2 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar.
Flexural Strength 70.0 MPa
10200 psi
SAE J949
Azdel SuperLite® SL552000-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness)
AZDEL SuperLite® SL552000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Strength 70.0 MPa
10200 psi
Plastcom SLOVALEN PC 91 T 30 PP, 30% mineral filling
FeaturesModified copolymer PP for injection moulding with the content of 30% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu..
Flexural Strength 70.0 MPa
10200 psi
ASTM D790
A. Schulman POLYFORT™ FPP 1220 Glass Filled Chemically Coupled Impact Copolymer Polypropylene
DescriptionPolyfort® FPP 1220 is a 20% glass filled chemically coupled impact copolymer polypropylene product.Information provided by A. Schulman.
Flexural Strength 70.0 MPa
10200 psi
ISO 178
Ascend Performance Materials Vydyne® 75HF Nylon 66/6, Heat Stabilized, DAM
Vydyne® 75HF is a medium-high-viscosity, heat-stabilized PA66/6 copolymer resin designed for extrusion applications. It is available in natural color only. Vydyne 75HF resin offers a well-balanced ..
Flexural Strength 70.3 MPa
10200 psi
ASTM D 790
RTP Company RTP 1505-55D Polyether-Ester Block Copolymer (TEEE/COPE), Glass Fiber