Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 117 MPa | 17000 psi | ASTM D790 |
PolyOne Nymax™ 600 A Zip 22 Natural Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Flexural Strength | 117 MPa | 17000 psi | ASTM D790 |
PolyOne Nymax™ 623 Zip 5 HS Black 13 Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Flexural Strength | 117 MPa | 17000 psi | |
Poco Graphite DFP-1C (Copper impregnated) Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
Flexural Strength | 117 MPa | 17000 psi | |
Pyrotek TS-84 Thermoset Electrical Insulation Product (Nema Grade: XX) Paper reinforcement, Phenolic Resin, Natural/Black Color. Good insulation in dry or humid conditions.Information provided by Pyrotek. |
|||
Flexural Strength | 117 MPa | 17000 psi | ASTM D790 |
Plaskolite Optix® DA Digital Acrylic Sheet Designed to provide optimal adhesion of UV curing inks without adhesion promoters, OPTIX DA is a continuously processed acrylic sheet specially formulated product for printing. OPTIX DA provides sup.. |
|||
Flexural Strength | 117 MPa | 17000 psi | ASTM D790 |
PolyOne Edgetek® AS-20CF/000 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 117 MPa | 17000 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000NL2 Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Flexural Strength | 117 MPa | 17000 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp KFL34 Acetal Copolymer LNP* Lubricomp* KFL34 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP f.. |
|||
Flexural Strength | 117 MPa | 17000 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP MFL36S PP LNP* LUBRICOMP* MFL36S is a compound based on Polypropylene resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Flexural Strength | 117 MPa | 17000 psi | DIN 54352 |
Schwartz Technical Plastics LAMIGAMID® 600 Polyoxymethylene Application: friction bearings, wear and sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Flexural Strength | 117 MPa | 17000 psi | ASTM D790 |
Techmer ES Electrablend® ABS CF10 A1 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 117 MPa | 17000 psi | ASTM D790 |
Techmer ES HiFill® PA6 E HS N Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Nucleating AgentFeatures: Heat Stabilized and NucleatedProcessing Method: ExtrusionTPCI# 9587102Information provided by TP Comp.. |
|||
Flexural Strength | 117 MPa | 17000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GB20 L BK 20% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 117 MPa | 17000 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon ZE0039 MODIFIED POYPHENYLENE LNP* Stat-kon* ZE0039 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 117 MPa | 17000 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DF002ERH PC LNP THERMOCOMP* DF002ERH is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Healthcare, Mold Release. |
|||
Flexural Strength | 117 MPa | 17000 psi | ASTM D790 |
Techmer ES Luriblend® PA6/6 ML2 HS NAT Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Molybdenum Disulfide Lubricant(2%)Features: Lubricated, Good Wear Resistance, Low Friction and Heat StabilizerAppear.. |
|||
Flexural Strength | 117 MPa | 17000 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DX06413H PC LNP* THERMOCOMP* DX06413H is a compound based on Polycarbonate resin containing 40% Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Flexural Strength | 117 MPa | 17000 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP GX05482 PSU (Asia Pacific) LNP* Thermocomp* GX05482 is a compound based on Polysulfone resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant. |
|||
Flexural Strength | 117 MPa | 17000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL HS2000X PPE+PS PPE+PS blend. 17% Mineral reinforced. Non-brominated, non-chlorinated FR system. UL94 V0 and 5VA listing. UL746C f1. Radiant panel listing. Dielectric strength. Dimensional stability. Suitable for E.. |
|||
Flexural Strength | 117 MPa | 17000 psi | ASTM D790 |
Asahi Kasei Thermylene® P6-30FG-0600R 30% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Strength | 117 MPa | 17000 psi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 113 Polypropylene, Glass Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 117 MPa | 17000 psi | ASTM D790 |
A. Schulman ComAlloy Lubrilon® 512 Polycarbonate, Glass Fiber/PTFE, UL Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Flexural Strength | 117 MPa | 17000 psi | ASTM Test |
BASF Ultramid® 1000-2 NF2001 PA66 (Dry) Ultramid 1000-2 NF2001 is a general purpose PA6/6. |
|||
Flexural Strength | 117 MPa | 17000 psi | ASTM Test |
BASF Ultramid® 1003-2 NF2002 PA66 (Dry) Ultramid 1003-2 NF2002 is a general purpose, heat stabilized nylon 6/6. |
|||
Flexural Strength | 117 MPa | 16900 psi | ASTM D790 |
Polymer Resources PPX-FRG10 Modified PPO, UL 94 V-1, 10% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 117 MPa | 17000 psi | ASTM D790 |
Sumitomo Bakelite Sumikon® PM-6430 Glass-Filled Phenolic, Compression Grade Sumikon PM-6430 black Phenolic is a two stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional sta.. |