Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 800 - 1000 MPa | 116000 - 145000 psi | Longitudinal |
Goodfellow Carbon/Vinyl Ester Rod Carbon Fiber - Vinyl ester MatrixInformation provided by Goodfellow. |
|||
Flexural Strength | 800 - 1000 MPa | 116000 - 145000 psi | Longitudinal |
Goodfellow Carbon/Vinyl Ester Tube Carbon Fiber - Vinyl ester MatrixInformation provided by Goodfellow. |