Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 103 MPa | 14900 psi | 1.3 mm/min; ASTM D790 |
PolyOne Gravi-Tech™ GRV-NY-027-SS-BLK-F Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Flexural Strength | 103 MPa | 14900 psi | ASTM D790 |
Polymer Resources PC-HM-FR2-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Flexural Strength | 103 MPa | 14900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® JK2000 PC+ABS (Asia Pacific) Lexan* JK2000 compound is a glass reinforced, non-Br and non-Cl FR polycarbonate blends designed for thinwall molding applications. |
|||
Flexural Strength | 103 MPa | 14900 psi | 1.3 mm/min; ASTM D790 |
PolyOne Edgetek® X TR2-10GF/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Flexural Strength | 103 MPa | 14900 psi | |
Cookson Group Plaskon® S-7P Epoxy Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, low viscosity epoxy encapsulant designed for packaging stress-sensitive semiconductor devices. It is specifically .. |
|||
Flexural Strength | 103 MPa | 14900 psi | |
Haysite 30000 Polyester BMC, 15% Glass Reinforced Haysite 30000 series bulk molding compound is a general purpose material. This compound can be compression, transfer, or injection molded. This material has good mechanical properties and can be pig.. |
|||
Flexural Strength | 103 MPa | 14900 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP QAP22S PA 6/10 (Asia Pacific) LNP* Lubricomp* QAP22S is a compound based on Nylon 6/10 resin containing PTFE, Aramid Fiber, Silicone. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
Flexural Strength | 103 MPa | 14900 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RAP22 PA 66 LNP* LUBRICOMP* RAP22 is a compound based on Nylon 66 resin containing 10% Aramid, 10% PTFE/Silicone. Added feature of this grade includes: Wear Resistant. |
|||
Flexural Strength | 103 MPa | 14900 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RL003 PA 66 LNP* LUBRICOMP* RL003 is a compound based on Nylon 66 resin containing 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Flexural Strength | 103 MPa | 14900 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP ZFL31XXC PPE+PS (Asia Pacific) LNP* Lubricomp* ZFL31XXC is a compound based on PPE+PS Blend resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | 103 MPa | 14900 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |
|||
Flexural Strength | 103 MPa | 14900 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Flexural Strength | 103 MPa | 14900 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Europe-Africa-Middle East) LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 103 MPa | 14900 psi | ISO 178 |
Solvay Specialty Polymers Lavanta® 5115 WH 011 Polyester, High Performance (HPP), 15% Glass Fiber Lavanta® 5115 WH011 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount .. |
|||
Flexural Strength | 103 MPa | 14900 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DX05475 PC LNP* THERMOCOMP* DX05474 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Flexural Strength | 103 MPa | 14900 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp IF002 PA 6/12 (Asia Pacific) LNP* Thermocomp* IF002 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Strength | 103 MPa | 14900 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly (Asia Pacific) LNP* Thermocomp* KF002L is a compound based on Acetal Homopolymer resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
Flexural Strength | 103 MPa | 14900 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MX95319 PP LNP* THERMOCOMP* MX95319 is a compound based on Polypropylene resin containing Proprietary Filler(s). |
|||
Flexural Strength | 103 MPa | 14900 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp OF004AER PPS LNP* Thermocomp* OF004AER is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.This data was supplied by SA.. |
|||
Flexural Strength | 103 MPa | 14900 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp OF004AER PPS (Asia Pacific) LNP* Thermocomp* OF004AER is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.This data was supplied by SA.. |
|||
Flexural Strength | 103 MPa | 14900 psi | ASTM D 790 |
SABIC Innovative Plastics Noryl N1150 PPE+HIPS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Strength | 103 MPa | 14900 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP NF001 PC+ABS (Asia Pacific) LNP* Thermocomp* NF001 is a compound based on PC+ABS Blend resin containing Glass Fiber. |
|||
Flexural Strength | 103 MPa | 14900 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66 LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing 40% Glass Bead. |
|||
Flexural Strength | 103 MPa | 14900 psi | |
Cosmic Plastics E4920 Mineral Filled Epoxy Molding Compound, Encapsulated Grade Data provided by the manufacturer. |
|||
Flexural Strength | 103 MPa | 14900 psi | |
Cosmic Plastics E4930 Mineral & Glass Filled Epoxy Molding Compound, Encapsulated Grade Data provided by the manufacturer. |
|||
Flexural Strength | 103 MPa | 14900 psi | ISO 178 |
Eurostar Staramide 6 70E3 PA6, 70% Mineral Filled, Injection Molded Staramide 6 70E3 is a 70% mineral filled high density, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Strength | 103 MPa | 14900 psi | 2 mm/min; ISO 178 |
Eurostar Starflam PK0049 PA6, Mineral Fiber Filled, Flame Retardant, Injection Molded Starflam PK0049 is a Free Flame Retardant Mineral Filled Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Strength | 103 MPa | 14900 psi | ASTM D790 |
Adell BS-10 Nylon 6, General Purpose Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 103 MPa | 14900 psi | ASTM D790 |
Unitika U-8000 U series resins are polymer alloys that are improved in resistance to oils and chemicals, the shortcoming of amorphous resins. They are transparent and have a greater moisture blocking property than.. |
|||
Flexural Strength | 103 MPa | 14900 psi | ASTM D790 |
Sumitomo Bakelite North America RX® 853G Fiberglass Reinforced Phenolic Novolac RX 853G is a fiberglass reinforced phenolic novolac compound, featuring dimensional stability, moderate impact resistance, and good strength and modulus.Information supplied by Sumitomo Bak North Am.. |