Mechanical Properties Metric English Comments
Flexural Strength 130 - 150 MPa
18900 - 21800 psi
Injection; ISO 178
Raschig Group 2557 AMC Polyester
Glass fiber reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, exceptional processability with short cycle time and low ..
Flexural Strength 120 - 150 MPa
17400 - 21800 psi
Injection; ISO 178
Raschig Group 6552 DAIP
Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi..
Flexural Strength 130 - 150 MPa
18900 - 21800 psi
At Rupture; ISO 178
Vyncolit X681 Novolac Phenolic
Glass fiber filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction. Tribological compound with PTFE additive.USES: Water pump seals and self-lubrica..
Flexural Strength 90.0 - 150 MPa
13100 - 21800 psi
Alliance S-26B Samarium Cobalt Magnetic Material
Flexural Strength 90.0 - 150 MPa
13100 - 21800 psi
Alliance S-28A Samarium Cobalt Magnetic Material
Flexural Strength 90.0 - 150 MPa
13100 - 21800 psi
Alliance S-28B Samarium Cobalt Magnetic Material
Flexural Strength 90.0 - 150 MPa
13100 - 21800 psi
Alliance S-30A Samarium Cobalt Magnetic Material
Flexural Strength 90.0 - 150 MPa
13100 - 21800 psi
Alliance S-30B Samarium Cobalt Magnetic Material
Flexural Strength 90.0 - 150 MPa
13100 - 21800 psi
Alliance S-28H Samarium Cobalt Magnetic Material
Flexural Strength 90.0 - 150 MPa
13100 - 21800 psi
Alliance S-32 Samarium Cobalt Magnetic Material
Flexural Strength 90.0 - 150 MPa
13100 - 21800 psi
Alliance S-26H Samarium Cobalt Magnetic Material
Copyright © lookpolymers.com All Rights Reserved