Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 88.0 - 110 MPa | 12800 - 16000 psi | ASTM D790 |
Proto3000 Accura® 55 Plastic Stereolithography (SLA) Prototyping Polymer Simulate the look and feel of molded ABS with this tough and versatile plastic.Features:Durable and rigid materialLook and feel of molded ABSHigh accuracy with less distortionHigh production speedLo.. |
|||
Flexural Strength | 75.0 - 110 MPa | 10900 - 16000 psi | ASTM D790-03 |
Proto3000 Objet Digital Materials™ DM_8310 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide.. |
|||
Flexural Strength | 75.0 - 110 MPa | 10900 - 16000 psi | ASTM D790-03 |
Proto3000 Objet Digital Materials™ DM_8320 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide.. |
|||
Flexural Strength | 75.0 - 110 MPa | 10900 - 16000 psi | ASTM D790-03 |
Proto3000 Objet Digital Materials™ DM_8330 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide.. |
|||
Flexural Strength | 80.0 - 110 MPa | 11600 - 16000 psi | ASTM D790-03 |
Proto3000 Objet Digital Materials™ DM_Dots_7513 Transparent Prototyping Polymer Primary material: FullCure720Secondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide t.. |
|||
Flexural Strength | 80.0 - 110 MPa | 11600 - 16000 psi | ASTM D790-03 |
Proto3000 Objet FullCure720 Transparent Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Flexural Strength | 75.0 - 110 MPa | 10900 - 16000 psi | ASTM D790-03 |
Proto3000 Objet VeroBlack FullCure870 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Flexural Strength | 75.0 - 110 MPa | 10900 - 16000 psi | ASTM D790-03 |
Proto3000 Objet VeroClear FullCure810 Information provided by Proto3000 for their protoyping engineering services. |
|||
Flexural Strength | 75.0 - 110 MPa | 10900 - 16000 psi | ASTM D790-03 |
Proto3000 Objet VeroGray FullCure850 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Flexural Strength | 90.0 - 110 MPa | 13100 - 16000 psi | Compression; ISO 178 |
Raschig Group 5553 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Flexural Strength | 90.0 - 110 MPa | 13100 - 16000 psi | Injection; ISO 178 |
Raschig Group DECAL® 2061 Phenolic Wood flour reinforced phenolic molding compound. Good electrical properties, chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals and PCAs and .. |
|||
Flexural Strength | 90.0 - 110 MPa | 13100 - 16000 psi | Injection; ISO 178 |
Raschig Group DECAL® 5431 Phenolic Organically and inorganically filled phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/.. |
|||
Flexural Strength | 90.0 - 110 MPa | 13100 - 16000 psi | Compression; ISO 178 |
Raschig Group MELOPAS® 156 MF Melamine Glass fiber reinforced Melamine molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 200.. |
|||
Flexural Strength | 90.0 - 110 MPa | 13100 - 16000 psi | Injection; ISO 178 |
Raschig Group MELOPAS® 6605 MP Melamine Cellulose reinforced Melamine molding compound. Very good electrical properties, excellent surface hardness, good mechanical strength and heat resistance, good wear and UV-stability, good gliding be.. |
|||
Flexural Strength | 80.0 - 110 MPa | 11600 - 16000 psi | Compression; ISO 178 |
Raschig Group MELOPLAS® 152 MF Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al.. |
|||
Flexural Strength | 80.0 - 110 MPa | 11600 - 16000 psi | Compression; ISO 178 |
Raschig Group MELOPLAS® 181.5 MF Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. Very good electrical properties, high surface hardness, good mechanical strength, high UV and heat resis.. |
|||
Flexural Strength | 90.0 - 110 MPa | 13100 - 16000 psi | At Rupture; ISO 178 |
Vyncolit 2923 W Novolac Phenolic Mineral filled phenolic molding compound with excellent heat resistance and dimensional stability.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Flexural Strength | 90.0 - 110 MPa | 13100 - 16000 psi | At Rupture; ISO 178 |
Vyncolit 2723 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent mechanical, thermal and dielectric properties. I2/FO classified under NF F 16-101 (Fire & Smoke classification).USES: Circuit bre.. |
|||
Flexural Strength | 88.0 - 110 MPa | 12800 - 16000 psi | ASTM D790 |
3D Systems Accura® 55 Plastic for SLA® Systems Simulate the properties and appearance of molded ABS. For use with solid-state stereolithography (SLA®) systems.ApplicationsAutomotive interior componentsShort-run production partsElectronic compon.. |
|||
Flexural Strength | 96.5 - 110 MPa | 14000 - 16000 psi | ASTM D790 |
Cast Nylons Nycast® RX Solid Lubricant Filled Red Cast Nylon 6 NYCAST® RX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti.. |
|||
Flexural Strength | 96.5 - 110 MPa | 14000 - 16000 psi | |
Bulk Molding Compounds BMC 102 Glass Filled Thermoset Polyester BMC 102 is a medium strength, glass fiber reinforced molding compound that meets Ford Specification ESF-M3D56-A. It can be supplied in bulk or extruded in pre-weighed slugs and is well suited for in.. |
|||
Flexural Strength | 82.7 - 110 MPa | 12000 - 16000 psi | |
Bulk Molding Compounds BMC 350 Thermoset Polyester, Medium Impact BMC 350 is a cosmetic and appliance grade material with excellent heat and stain resistant properties. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical ap.. |
|||
Flexural Strength | 82.7 - 110 MPa | 12000 - 16000 psi | |
Bulk Molding Compounds BMC 605LWR Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605LWR is a mineral filled, glass fiber reinforced polyester bulk molding compound suitable for compression, transfer and stuffer injection molding. It is designed to provide improved wear resis.. |
|||
Flexural Strength | 82.7 - 110 MPa | 12000 - 16000 psi | |
Bulk Molding Compounds BMC A30 General Purpose Molding Compound BMC A30 is a general purpose molding compound with good dimensional stability. Due to the excellent flow and controlled reactivity, BMC A30 is well suited for injection, transfer or compression mol.. |
|||
Flexural Strength | 82.7 - 110 MPa | 12000 - 16000 psi | |
Bulk Molding Compounds BMC A30-3021 General Purpose Molding Compound BMC A30-3021 is a low shrink, general purpose molding compound formulated for the lighting industry. A30-3021 is temperature stabilized for use in elevated temp. lighting applications. Due to the .. |
|||
Flexural Strength | 103 - 110 MPa | 15000 - 16000 psi | |
Bulk Molding Compounds BMC SLC 1000 Glass Reinforced Polyester BMC SLC 1000 is a medium strength, low-cost, glass reinforced polyester compound with adjustable shrinkage. It is V-0 flame arc and track resistant. UL® recognized. This material was formerly known.. |
|||
Flexural Strength | 70.0 - 110 MPa | 10200 - 16000 psi | ISO 178 |
Bulk Molding Compounds tetra-DUR F 4209 Bulk Molding Compound Highest Arc resistanceTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), therm.. |
|||
Flexural Strength | 82.7 - 110 MPa | 12000 - 16000 psi | |
Bulk Molding Compounds BMC 1050 Thermoset Polyester BMC 1050 is a cosmetic, appliance grade material with superior heat stability. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical applications are toaster e.. |
|||
Flexural Strength | 75.0 - 110 MPa | 10900 - 16000 psi | ASTM D790-03 |
Proto3000 Objet VeroWhitePlus FullCure835 Rigid Opaque Prototyping Polymer Information provided by Proto3000 for their protoyping engineering services. |
|||
Flexural Strength | 96.5 - 110 MPa | 14000 - 16000 psi | |
Bulk Molding Compounds BMC T15(GPT) General Purpose Molding Compound BMC T15(GPT) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GPT) is well suited for injection, transfer or compression.. |