Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 115 MPa | 16700 psi | |
Plastcom SLOVAMID 6 NGR PA6, basic type FeaturesPA 6 for injection moulding, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, faste.. |
|||
Flexural Strength | 115 MPa | 16700 psi | 1.5mm/min; ISO 178:2001 |
Nylacast Nylube GF Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant), Glass Filled For applications requiring higher compressive strength the NYLUBE GF masterbatch incorporates hollow glass ovule, designed to float and evenly distribute through the polymerising polymer. The glass .. |
|||
Flexural Strength | <= 115 MPa | <= 16700 psi | ISO 178 |
Polykemi AB POLYblend 85FS GF10 PC/ABS-Blend, Glass Fiber reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 115 MPa | 16700 psi | ASTM D790 |
Nilit Polynil® P120 Medium Viscosity Nylon 66 Description: Medium viscosityApplication: MonofilamentInformation provided by NILIT. |
|||
Flexural Strength | <= 115 MPa | <= 16700 psi | ISO 178 |
Polykemi AB POLYshine PBT D234 GF30 FR PBT, Glass-Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Flexural Strength | 115 MPa | 16700 psi | |
Lehmann & Voss LUVOCOM® 1-7985 Polyamide 66, with aramid reinforcement and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Improved heat resistance.Control disks, cams, sliding elements and o.. |
|||
Flexural Strength | 115 MPa | 16700 psi | ISO 178 |
Kuraray Genestarâ„¢ N1000A-M41 Nylon Standard unreinforced injection grade. Main features:Low water absorptionChemical ResistanceExamples of application are:Friction and wear applicationGear and Wheel |
|||
Flexural Strength | 115 MPa | 16700 psi | ASTM D790 |
Solvay TECHNYL® C 50 H2 PA6, DRY Description: TECHNYL® C 50H2 is a unreinforced melamine cyanurate flame retarded polyamide 6. This product is heat stabilized and can be used for injection molding and extrusion processes. This p.. |
|||
Flexural Strength | 115 MPa | 16700 psi | ISO 178 |
Solvay Technyl® C206F Unfilled, Fast Cycle Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Flexural Strength | 115 MPa | 16700 psi | ISO 178 |
Solvay TECHNYL® PSB 286 PA6, DRY Description: Unreinforced polyamide PA6, with very good lubrication, standard for fast injection cycles, for injection molding.Available in: North AmericaProduct Applications: This grade has high fl.. |
|||
Flexural Strength | 115 MPa | 16700 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Conditioned) Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin.. |
|||
Flexural Strength | 115 MPa | 16700 psi | ASTM D790 |
Techmer ES HiFill® PA6 E40 Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 115 MPa | 16700 psi | ASTM D790 |
Techmer ES HiFill® PA6 L LE MB Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Lubricated, Heat Stabilized and Low ExtractablesAppearance: Colors AvailableTPCI# 7964102Information provide.. |
|||
Flexural Strength | 115 MPa | 16700 psi | ASTM D790 |
Techmer ES HiFill® PA6 L UV (Dry) Availability: North AmericaForms: PelletsAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 115 MPa | 16700 psi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp KF003 Acetal Copoly LNP* Thermocomp* KF003 is a compound based on Acetal Copolymer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 115 MPa | 16700 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS LNP* Thermocomp* Lexan_JK500 compound is a 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications. |
|||
Flexural Strength | 115 MPa | 16700 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS (Asia Pacific) 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications. |
|||
Flexural Strength | 115 MPa | 16700 psi | ISO Data |
Styrolution Terblend® N NG-04 20% Glass Filled ABS/PA6 (Dry) Terblend N NG-04 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, low mold shrinkage and high heat resistance.Information provided by STYROLUTION, which is a joint ven.. |
|||
Flexural Strength | 115 MPa | 16700 psi | ISO 178 |
Borealis GB205U Polypropylene Compound, Glass Fiber Reinforced GB205U is a 20% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Thi.. |
|||
Flexural Strength | 115 MPa | 16700 psi | ASTM D790 |
Plenco 6582 Phenolic, Briquette, Transfer Molded PLENCO 06582 is a rubber modified phenolic molding compound, offering excellent heat resistant properties, along with improved mechanical strength at elevated temperatures. UL recognized under compo.. |
|||
Flexural Strength | 115 MPa | 16700 psi | ISO 178 |
Polyram PlusTek PA700BL10 Nylon 6.6 for Injection Molding, UV Stabilized UV Stabilized Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Flexural Strength | 115 MPa | 16700 psi | ISO 178-93 |
Wellman Wellamid® GFT1699-WBK1 13% Glass Fiber Reinforced, Weatherable Black Nylon 66 Description: Glass Fiber Reinforced, Weatherable Black Nylon 66Information provided by Wellman. |
|||
Flexural Strength | 115 MPa | 16700 psi | ASTM-D790 |
Polyram RamShine PV300G6 ABS, 30% Glass Fiber 30% glass fiber reinforced, heat resistance and minimal mold shrinkage ABS for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Strength | 115 MPa | 16700 psi | ASTM D790 |
A. Schulman SCHULAMID® 66 MV3FR Flame Retardant Nylon 6/6 Information provided by A. Schulman. |
|||
Flexural Strength | 115 MPa | 16700 psi | 2 mm/min; ISO 178 |
Eurostar Staramide BG4ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG4ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Strength | 115 MPa | 16700 psi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 104 Polypropylene, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 115 MPa | 16700 psi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 123 Polypropylene, Glass Reinforced, Chemically Coupled, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 115 MPa | 16700 psi | at max force; ISO 178 |
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Conditioned) Description: Halogen- and phosphorus-free injection-molding grade with very high rigidity, low smoke density and outstanding electrical properties.Information provided by BASF |