Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 158.6 MPa | 23000 psi | Lengthwise; IPC-TM-650.2.4.4 |
Park Electrochemical Nelco® NH9350 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Flexural Strength | 158.6 MPa | 23000 psi | Lengthwise; IPC-TM-650.2.4.4 |
Park Electrochemical Nelco® NX9240 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Flexural Strength | 158.6 MPa | 23000 psi | Lengthwise; IPC-TM-650.2.4.4 |
Park Electrochemical Nelco® NX9245 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1033THL Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Polymer Resources NY66-G13-[color]-H Nylon 66, 13% Glass Reinforced, Heat Stabilized Nylon 66, 13% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo.. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Polymer Resources NY66-IM1-G13-[color]-H Nylon 66, 13% Glass Reinforced, Toughened and Heat Stabilized Nylon 66, 13% Glass Reinforced, Toughened, Lubricated, and Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes.. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790-1 |
Premix Premi-Glas® 8201-24 Glass Reinforced Polyester SMC
(discontinued **) Description: Premi-Glas® 8201-24 is a low profile glass reinforced polyester Sheet Molding Compound designed for body panel applications.Key features and benefits: Compatible with in-mold coatings,.. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1033TL Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago. |
|||
Flexural Strength | 159 MPa | 23000 psi | |
XXX Phenolic Laminate Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided b.. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Haysite H320 Polyester Composite A thermoset polyester composite that offers superior energy efficiency, temperature control, and durability for high temperature mold and platen thermal applications. A proven, cost effective produ.. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF/M36 HS BK 36% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 36% Filler by Weight and Mineral Filler, 36% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF15 TL5 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by Weight Additive: PTFE Lubricant (5%)Features: LubricatedAppearance: Natural ColorInformation p.. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Techmer ES Statiblend® PA6/6 GF20 AS BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Lubricant, Antistatic and Heat StabilizerFeatures: Antistatic, Heat Stabilized and Lubricate.. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Techmer ES HiFill® ABS GF30 HT 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
A. Schulman SCHULADUR® A GF15 15% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Strength | 159 MPa @Temperature 22.8 °C |
23000 psi @Temperature 73.0 °F |
ASTM D790 |
Ensinger TECATOR™ TI 5031 Polyamide-imide (PAI), Bearing Grade TECATOR™ is a high performance melt processable polyamideimide that maintains its excellent mechanical and wear properties in temperature environments exceeding 500°F. Stock shapes from Ensinger .. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Asahi Kasei Thermylene® P7-40FG-0600 40% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Strength | 159 MPa | 23000 psi | |
Anderman Ceramics EM60 Mullite Synthetic mullite available in rod, tube, sheaths and insulators up to 10 ft (3 m) long with diameters 0.3" to 19".Information provided by Anderman Ceramics. |
|||
Flexural Strength | 159 - 172 MPa | 23000 - 25000 psi | |
Bulk Molding Compounds BMC 1412 Flame and Track Resistant BMC 1412 is an extremely versatile material. Flame and track resistant, low shrink for close dimensional control and surface smoothness, high physical properties. Developed for injection molding, bu.. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Quadrant EPP Duratron® PAI T4301 Polyamide-imide, extruded bearing grade (ASTM Product Data Sheet) |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Quadrant EPP Ketron® CM CA30 PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to ho.. |