Mechanical Properties Metric English Comments
Flexural Strength 140 - 160 MPa
20300 - 23200 psi
Injection; ISO 178
Raschig Group 2568 AMC
Glass fiber-reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, heat resistant up to 500°C for short time - usable for s..
Flexural Strength 140 - 160 MPa
20300 - 23200 psi
Injection; ISO 178
Raschig Group 2572 AMC
Glass fiber reinforced Polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, good abrasion stability, high flame retardance in combin..
Flexural Strength 120 - 160 MPa
17400 - 23200 psi
Injection; ISO 178
Raschig Group 5562 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
Flexural Strength 120 - 160 MPa
17400 - 23200 psi
Injection; ISO 178
Raschig Group 5563 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
Flexural Strength 140 - 160 MPa
20300 - 23200 psi
Injection; ISO 178
Raschig Group DECAL® 666/8/2B Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meets the allowe..
Flexural Strength 140 - 160 MPa
20300 - 23200 psi
Injection and Compression; ISO 178
Raschig Group EPOXIDUR® 3581 T-1 EP Epoxy, Molded, Glass Fiber Filler
Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very ..
Flexural Strength 140 - 160 MPa
20300 - 23200 psi
Injection; ISO 178
Raschig Group SURAPLAST UPA 63 UP
Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for..
Flexural Strength 140 - 160 MPa
20300 - 23200 psi
At Rupture; ISO 178
Vyncolit 2950 W Novolac Phenolic
Mineral and glass fiber filled phenolic molding compound with a very high strain to failure in flexure. UL listed.USES: Armature insulation.Information provided by Vyncolit, a Sumitomo Bak Group