Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
PolyOne LubriOne™ NL-30CF/15T Black Polyamide 612 (Nylon 612) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
Oxford Polymers Oxnilon 6-33GF 33% Glass Fiber Filled Nylon 6 for Injection Molding 33% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Flexural Strength | 269 MPa @Temperature 23.9 °C |
39000 psi @Temperature 75.0 °F |
Dry; 8HS form; ASTM D790 |
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, ENKA Reinforced Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel.. |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
LNP Thermocomp® UF-1006 HS Polyphthalamide, Glass Fiber Reinforcement
(discontinued **) Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti.. |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
LNP Thermocomp® EF-1006 BK8-114 Polyetherimide, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Flexural Strength | 269 MPa | 39000 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP OCL36EXP PPS - LINEAR LNP* LUBRICOMP* OCL36EXP is a compound based on Linear PPS containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include; Wear Resistant, Electrically Conductive. |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® BR42B 40% glass fiber reinforced polyphenylene sulfide compound is specially formulated to provide low coefficient of friction and reduced wear rate for use in applications requiring low s.. |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
Techmer ES HiFill® PA4/6 GF30 TL15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and PTFE LubricantFeatures: Heat Stabilized and LubricatedInfo.. |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 L 50% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
Techmer ES HiFill® PEEK GF30 HF 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: High FlowInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
Techmer ES Luriblend® PA6/6 GF40 ML2 HS BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(5%)Features: Lubricated and Heat Stabiliz.. |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
Techmer ES Luriblend® PA6/6 GF43 ML2 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 43% Filler by WeightAdditive: Molybdenum Disulfide Lubricant(2%)Features: LubricatedInformation provided by TP Composites,.. |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
Techmer ES Luriblend® PPA CF30 TL15 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, High Heat Resistance and Low.. |
|||
Flexural Strength | 269 MPa | 39000 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI (Asia Pacific) LNP THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 269 MPa | 39000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON OE006C1 PPS - Linear LNP* STAT-KON* OE006C1 is a compound based on PPS - Linear resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 269 MPa | 39000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RC004SXC PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RC004SXC is a compound based on PA66 resin containing Carbon Fiber. Added features include: Electrically Conductive, Heat Stabilized. |
|||
Flexural Strength | 269 MPa | 39000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RC004SXS PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RC004SXS is a compound based on PA 66 resin containing Carbon Fiber. Added features include; Heat Stabilized, Electrically Conductive. |
|||
Flexural Strength | 269 MPa @Temperature 23.0 °C |
39000 psi @Temperature 73.4 °F |
DAM; ASTM D790 |
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612
(Unverified Data**) Zytel® 77G43L BK031 is a 43% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Strength | 269 MPa | 39000 psi | ASTM D790 |
PolyOne Edgetek® AM-20CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 269 MPa @Temperature 23.0 °C |
39000 psi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry
(discontinued **) Amodel A-4133L polyphthalamide (PPA) is a 33% glass reinforced resin designed to offer high crystallinity when molded in water-cooled molds. Key properties include high heat resistance, reduced outg.. |