Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced Polyetherimide, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Quadrant EPP Duratron® PBI CU60 Polybenzimidazole, unfilled, compression molded (ASTM Product Data Sheet) Duratron® PBI is the highest performance engineering plastic available from Quadrant EPP. It offers the highest mechanical properties of any thermoplastic above 400° F (205° C). Duratron® PBI .. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
PolyOne Lubri-Tech™ NL-30CF/10T-2S Nylon 6/12, Carbon Fiber Reinforced, PTFE Lubricated
(discontinued **) Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
PolyOne Edgetek® SF-20CF/000 Polyphenylene Sulfide (PPS)
(discontinued **) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Techmer ES Electrafil® J-1305/CF/30/TF/15 NAT PPS |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF30 FR BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedAppear.. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF/M40 HS L 40% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedTPCI# 7395102Informat.. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF/M40 ML2 GY 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Molybdenum Disulfide Lubricant and He.. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF33 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: LubricatedTPCI# 8682101Information provided by TP Composite.. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF33 L UV 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceTPCI# 82.. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Techmer ES Luriblend® PA6/6 GF30 TS1 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R.. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Teknor Apex Chemlon® 233 GVH Nylon 6, 33% Glass Fiber Reinforced Features: Flame Retardant; Good Stiffness; High Strength Processing Method: Injection Method Forms: Pellets Additive: Flame RetardantInformation Provided by Teknor Apex |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Techmer ES HiFill® PA4/6 GF25 HS NAT 25% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: Natural ColorInformation p.. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF33 HS L GY 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
A. Schulman SCHULADUR® B GF30 30% Glass Fiber Reinforced PET Information provided by A. Schulman. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
A. Schulman SCHULAMID® 6 GF15H 30% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
A. Schulman SCHULAMID® 6 GF15H 30% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
A. Schulman SCHULADUR® B GF30 30% Glass Fiber Reinforced PET Information provided by A. Schulman. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
A. Schulman SCHULAMID® 6 GF15H 30% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Flexural Strength | 221 MPa | 32000 psi | IPC TM-650 2.4.4 |
Arlon GenClad™ 280 Low Loss Thermoset Bond-Ply Low loss Ceramic-Filled Thermoset/Thermoplastic Hybrid SystemRivals PTFE laminate electrical performance in a Halogen-Free systemLight weight material relative to standard laminate materialsOptimal .. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
A. Schulman SCHULADUR® B GF30 30% Glass Fiber Reinforced PET Information provided by A. Schulman. |