Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 225.63 MPa | 32725 psi | |
Shinil Chemical SHINCON PEI-CNT Magazine Rack Magazine Rack is used to transfer, handle, and bake lead frame or PCB substrate in semiconductor and LED packaging assembly process. Current Metal Magazine is made of anodized aluminum which is exp.. |
|||
Flexural Strength | 225.63 MPa | 32725 psi | |
Shinil Chemical SHINCON PPS Electro Conductive Polymer SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's .. |
|||
Flexural Strength | 225.63 MPa | 32725 psi | |
Shinil Chemical SHINCON PPS-CNT LCD Rack LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b.. |
|||
Flexural Strength | 225.63 MPa | 32725 psi | |
Shinil Chemical SHINNANO PA-6 Polymer Nanocomposite Air Intake Module SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using.. |