Polymer Property : Flexural Strength = 33.1 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 33.1 MPa
4800 psi
ASTM D790
PolyOne Maxxam™ FR PP 307 Polypropylene, Unspecified (PP, Unspecified)
Information provided by PolyOne
Flexural Strength 33.1 MPa
4800 psi
ASTM D790
Quadrant EPP Proteus® O & P Grade, Natural Homopolymer Polypropylene (ASTM Product Data Sheet)
Flexural Strength 33.1 MPa
4800 psi
ASTM D790
Quadrant EPP Proteus® PP Natural Co-Polymer Polypropylene (ASTM Product Data Sheet)
Flexural Strength 33.1 MPa
4800 psi
ASTM D790
Quadrant EPP Proteus® PP, Black Homopolymer Polypropylene (ASTM Product Data Sheet)
High impact resistance strength Better resistance to cracking at low temperatures than Homopolymer Polypropylene More pliable than homopolymer Meets food handling guidelines Chemical- and corrosion..
Flexural Strength 33.1 MPa
4800 psi
ASTM D790
Quadrant EPP Proteus® PP, Natural Homopolymer Polypropylene (ASTM Product Data Sheet)
Flexural Strength 33.1 MPa
4800 psi
ASTM D790
Quadrant EPP Proteus® PP, ProKnob Finish Natural Homopolymer Polypropylene (ASTM Product Data Sheet)
High impact resistance strength Better resistance to cracking at low temperatures than Homopolymer Polypropylene More pliable than homopolymer Meets food handling guidelines Chemical- and corrosion..
Flexural Strength 33.1 MPa
4800 psi
ASTM D790
Fiberfil® PP-60/VO/NH Polypropylene Homopolymer, Flame Retardant, non-halogenated, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Flexural Strength 33.1 MPa
4800 psi
ASTM D790
Chesterton ARC BX1 Sliding Wear Compound
Description: An advanced contractor grade ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is normally applied at..
Flexural Strength 33.1 MPa
4800 psi
ASTM D790
Ensinger Tecatron® XP-84 Compression Molded PPS Compound, 30% Graphite Filled
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p..
Flexural Strength <= 33.1 MPa
<= 4800 psi
ASTM D790
Arkema Group Solarkote® P-610 Acrylic
PVC Capstock, clear, low glossInformation provided by Arkema Group
Flexural Strength <= 33.1 MPa
<= 4800 psi
ASTM D790
Arkema Group Solarkote® P-600 Acrylic
PVC Capstock, clear, high glossInformation provided by Arkema Group
Flexural Strength <= 33.1 MPa
<= 4800 psi
ASTM D790
Arkema Group Solarkote® P-601 Acrylic
PVC Capstock, white, high glossInformation provided by Arkema Group
Flexural Strength <= 33.1 MPa
<= 4800 psi
ASTM D790
Arkema Group Solarkote® P-611 Acrylic
PVC capstock, white, low glossInformation provided by Arkema Group
Flexural Strength 33.1 MPa
4800 psi
ASTM D790
Adell RZ-14 Copolymer Polypropylene, 20% Calcium Carbonate Filled
Data provided by Adell Plastics, Inc.
Flexural Strength 33.1 MPa
4800 psi
ASTM D790
Quadrant EPP Proteus® White Homopolymer Polypropylene (ASTM Product Data Sheet)