Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 2.50 MPa | 363 psi | @ 25 kg/m<sup>2</sup>; ASTM DC201 |
Samsung Cheil Industries Starex® SG-501 Expandable Polystyrene (EPS) High Expansion Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 2.50 MPa | 363 psi | @ 25 kg/m<sup>2</sup>; ASTM DC201 |
Samsung Cheil Industries Starex® SG-501 Expandable Polystyrene (EPS) High Expansion Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 2.50 MPa | 363 psi | SAE J949 |
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (9 mm Molded Thickness) AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Strength | 2.50 MPa | 363 psi | SAE J949 |
Azdel SuperLite® SL552000-100 PP Resin Matrix / 55% Glass Fiber (10 mm Molded Thickness) AZDEL SuperLite® SL552000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Strength | 2.50 MPa | 363 psi | SAE J949 |
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (8 mm Molded Thickness) AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |