Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 37.0 MPa | 5370 psi | |
Plastcom SLOVALEN PC 73 T 15-1M PP, 15% mineral filling, UV stable FeaturesModified PP copolymer for injection moulding with the content of 15 % mineral filler, uv stabilized, good scratch resistance, low odor and very good flowability with good dimensional stabili.. |
|||
Flexural Strength | 37.0 MPa | 5370 psi | |
Plastcom SLOVALEN PH 51 T 60 PP, 60% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 60% microground, floated, chemically modified talc. General application in all industry. Delivered in natural mode and in t.. |
|||
Flexural Strength | 37.0 MPa | 5370 psi | |
Plastcom SLOVALEN PH 99 GB 20 PP, 20% glass beads, mod. of mech. prop. FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Flexural Strength | <= 37.0 MPa | <= 5370 psi | ISO 178 |
Polykemi AB POLYfill PP CIP6015F Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 37.0 MPa | 5370 psi | ASTM D790 |
Proto3000 Duraform® GF Selective Laser Sintering (SLS®) Prototyping Polymer Description: Glass-filled polyamide (nylon) material for real-world physical testing and functional useFeatures:Excellent mechanical stiffnessElevated temperature resistanceDimensionally stableEasy-.. |
|||
Flexural Strength | >= 37.0 MPa | >= 5370 psi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM 825 High Impact Polystyrene Grade 825 is a high impact polystyrene for injection molding. The polymer's ability to be molded on fast cycles with minimal stresses results in outstanding impact retention. It is used in such ap.. |
|||
Flexural Strength | <= 37.0 MPa | <= 5370 psi | ISO 178 |
Polykemi AB POLYfill PP CIP6015F VTUV Polypropylene, Mineral Reinforced, Heat and UV Stabilized Information provided by Polykemi AB |
|||
Flexural Strength | 37.0 MPa | 5360 psi | Injection molded; ASTM D790 |
Americas Styrenics STYRON™ A-TECH™ 6079 Ignition Resistant Polystyrene Resin
(discontinued **) STYRON™ A-TECH™ 6079 is an ignition resistant polystyrene (IRPS) resin designed specifically for consumer and business electronics applications that demand excellent aesthetics, along with a stron.. |
|||
Flexural Strength | 37.0 MPa | 5370 psi | ASTM D790 |
Ineos Nova FX510 Super High Impact Polystyrene
(discontinued **) Features: Extremely high impact strengthGood flexural strengthUL Classification 94 HBCustom colors availableApplications: Injection molding or extrusionSuitable replacement for some engineering resi.. |
|||
Flexural Strength | 37.0 MPa | 5370 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP ML004LS PP LNP* LUBRICOMP* ML004LS is a compound based on Polypropylene resin containing 20% PTFE. Added features of this matLNP* Lubricomp* ML004LS is a compound based on Polypropylene resin containing PTFE... |
|||
Flexural Strength | 37.0 MPa | 5370 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS (Europe-Africa-Middle East) LNP* Stat-loy* A3000T is a compound based on Acrylonitrile Butadiene Styrene resin. Added features of this material include: Antistat. |
|||
Flexural Strength | 37.0 MPa | 5370 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MX95318 PP LNP* THERMOCOMP* MX95318 is a compound based on Polypropylene containing Proprietary Filler(s). |
|||
Flexural Strength | 37.0 MPa | 5370 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON CD000 PS (Europe-Africa-Middle East) LNP* Stat-kon* CD000 is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 37.0 MPa | 5370 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp MFK42AS PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MFK42AS is a compound based on PP resin containing Glass Fiber, Mineral.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Strength | 37.0 MPa | 5370 psi | 2 mm/min; ISO 178 |
Eurostar Starpylen MFK42AS PP, Glass/Mineral Filled, Injection Molded Starpylen MFK42AS is a Mineral Filled, Glass Fiber Reinforced, Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Strength | 37.0 MPa | 5370 psi | ASTM D790 |
Entec Hypro™ PPH-CC10 Natural Homopolymer Polypropylene, 10% Calcium Carbonate Filled Information provided by Entec |
|||
Flexural Strength | 37.0 MPa | 5370 psi | ASTM D790 |
3D Systems DuraForm® GF Glass Filled Nylon For use with all selective laser sintering (SLS®) systems.ApplicationsHousings and enclosuresConsumer sporting goodsAppropriate for low- to mid-volume rapid manufacturingParts requiring machining o.. |
|||
Flexural Strength | 37.0 MPa | 5370 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336W10L1 Wollastonite Reinforced |
|||
Flexural Strength | 37.0 MPa | 5370 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339C10L1 Calcium Reinforced |
|||
Flexural Strength | 37.0 MPa | 5370 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339C20L Calcium Reinforced |
|||
Flexural Strength | 37.0 MPa | 5370 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339C20L1 Calcium Reinforced |
|||
Flexural Strength | 37.0 MPa | 5370 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339C30L Calcium Reinforced |
|||
Flexural Strength | 37.0 MPa | 5370 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339C30L1 Calcium Reinforced |
|||
Flexural Strength | 37.0 MPa | 5370 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339C40L Calcium Reinforced |
|||
Flexural Strength | 37.0 MPa | 5370 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339C40L1 Calcium Reinforced |
|||
Flexural Strength | 37.0 MPa | 5370 psi | ISO 178 |
Azoty Tarnow™ TARNOFORM 300 HI4 POM High impact strength grade, high damping capacity.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Flexural Strength | 37.0 MPa | 5370 psi | 0.1 in/min; ASTM D790 |
Ineos Nova Zyntar® 351 High Performance Flame Retardant Polystyrene
(discontinued **) High Vicat and heat reflection temperature, Custom colorsApplications: Injection molding, Gas-assist injection molding, Structural foam, TV cabinets, Electronic enclosuresThis is an impact grade of .. |
|||
Flexural Strength | 37.0 MPa | 5370 psi | |
Plastcom SLOVALEN PH 91 C 20 PP, 20% mineral filling FeaturesModified homopolymer and copolymer PP for injection moulding with the contenct of 20% microground, chemically modified talc. Increased strength, rigidity and thermal application up to 100°C.. |