Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 37.9 MPa | 5500 psi | ASTM D790-95 |
Multibase Multi-Pro® 3216 CUW BLK Polypropylene Multi-Pro 3216 CUW BLK is well suited for resin furniture requiring high impact strength and stiffness at moderate cost.Data provided by Multibase. |
|||
Flexural Strength | 37.9 MPa | 5500 psi | ASTM D790 |
PolyOne LubriOne™ ATH-000/18T 2S Acetal (POM) Homopolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Strength | 37.9 MPa | 5500 psi | ASTM D790 |
PolyOne Trilliant™ HC X HC5200-0025 RS Natural Polypropylene Copolymer (PP Copolymer) Information provided by PolyOne |
|||
Flexural Strength | 37.9 MPa | 5500 psi | ASTM D790 |
PolyOne Lubri-Tech™ AT-15GP/5T Acetal-Copolymer, PTFE Lubricated
(discontinued **) Description/Features:Graphite LubricatedPTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 37.9 MPa | 5500 psi | ASTM D790 |
PolyOne Edgetek® AS-10GF/000 FR Acrylonitrile Butadiene Styrene (ABS), Glass/Carbon Fiber Filled
(discontinue Description/Features:Glass/Carbon Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 37.9 MPa | 5500 psi | ASTM D790 |
Fiberfil® PP-60/FR Polypropylene Homopolymer, Flame Retardant, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 37.9 MPa | 5500 psi | ISO 178 |
Fiberfil® PP-60/TC/15/VO/ND Polypropylene Homopolymer, 15% Talc Filled, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 37.9 MPa | 5500 psi | ASTM D790 |
Kostat ICP-STAT ICS-1002 PP Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Flexural Strength | 37.9 MPa | 5500 psi | ASTM D 790 |
Styrolution PS 5410 HIPS Good printabilityGood environmental stress crack resistanceLow GelsTrims CleanlyLow Gloss (matte finish)Information provided by Styrolution |
|||
Flexural Strength | 37.9 MPa | 5500 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Strength | 37.9 MPa | 5500 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Strength | 37.9 MPa | 5500 psi | ASTM D790 |
Total PSI 935E Polystyrene Polystyrene 935E is a high impact polystyrene exhibiting exceptional toughness for sheet and thermoforming applications.This polymer is an excellent choice for cups, food packaging, custom sheet and.. |
|||
Flexural Strength | 37.9 MPa | 5500 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Strength | 37.9 MPa | 5500 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Strength | 37.9 MPa | 5500 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Strength | 37.9 MPa | 5500 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Strength | 37.9 MPa | 5500 psi | |
Anderman Ceramics EM80P Corundum Porous synthetic mullite with very high thermal shock. Available as tube, sheath, or rod up to 10 ft (3 m) long with diameters 0.3" to 20".Information provided by Anderman Ceramics. |
|||
Flexural Strength | 37.9 MPa | 5500 psi | ASTM D790 |
Adell RA-14 Copolymer Polypropylene, 20% Talc Filled Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 37.9 MPa | 5500 psi | ASTM D790 |
PolyOne Lubri-Tech™ AT-20GB/15T Acetal-Copolymer, Glass Bead Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Bead FilledPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 37.9 MPa | 5500 psi | ASTM D790 |
Asahi Kasei Thermofil P-10CC-Y488 10% Calcium Carbonate Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Strength | 37.9 MPa | 5500 psi | ASTM D790 |
PolyOne Edgetek® AS-10GB/000 Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled