Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | <= 41.0 MPa | <= 5950 psi | ISO 178 |
Polykemi AB POLYfill PPC K2040 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 41.0 MPa | 5950 psi | 0.1 in/min; 0.250" thickness; ASTM D-790B |
Chevron Phillips MA5350 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Floppy diskettesDurable household applicationsThin to medium parts that require a combination of high gloss and good toughnessFeatures:Low coeffi.. |
|||
Flexural Strength | 41.0 MPa | 5950 psi | 0.1 in/min; 0.250" thickness; ASTM D-790B |
Chevron Phillips MD6800 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Displays and retail product shelvingDurable household applicationsThin to medium thickness parts that require a combination of high flow and good.. |
|||
Flexural Strength | 41.0 MPa | 5950 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP CBL36XXC PS LNP* LUBRICOMP* CBL36XXC is a compound based on Polystyrene resin containing 30% Glass Bead and 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Flexural Strength | 41.0 MPa | 5950 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp CI001 PS LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the America.. |
|||
Flexural Strength | 41.0 - 46.0 MPa | 5950 - 6670 psi | ASTM D790M |
DSM Somos® 9120 Epoxy Photopolymer
(Unverified Data**) DescriptionDSM Somos® 9120 is a liquid photopolymer that produces robust, functional and accurate parts using stereolithography machines. The material offers superior chemical resistance, a wide p.. |
|||
Flexural Strength | 41.0 MPa | 5950 psi | ASTM D790 |
Kolon KOCETAL® EL306 Toughened Grade Acetal Resin Flexible grade. Applications: Flexible products. Information provided by API-Kolon. |
|||
Flexural Strength | 41.0 MPa | 5950 psi | at 5% strain; ASTM D790 |
Ineos Nova FX530 Impact Polystyrene Features: Excellent environmental stress crack resistanceExcellent Izod impact strengthUL Classification 94 HBBalanced physical propertiesApplications: ExtrusionThermoformingSelected injection moldi.. |
|||
Flexural Strength | 41.0 MPa | 5950 psi | ASTM D790 |
LG Chemical LUPOL HM-5204B High Modulus Polypropylene, 20% Polymer Alloy, High Strength, High Flow, High Modulus LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Flexural Strength | 41.0 MPa | 5950 psi | ISO 178 |
Lucite International Elvakon® 4461 Medium Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Flexural Strength | 41.0 MPa | 5950 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON CD000I PS (Asia Pacific) LNP* Stat-kon* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Flexural Strength | 41.0 MPa | 5950 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS LNP* STAT-LOY* A30009 is a compound based on ABS. Added features of this material include: Antistatic, Flame Retardant. |
|||
Flexural Strength | 41.0 MPa | 5950 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS (Asia Pacific) LNP* Stat-loy* A30009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant. Added features of this material include: Antistat, Flame Retardant. |
|||
Flexural Strength | 41.0 MPa | 5950 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS (Asia Pacific) LNP* Stat-loy* A3000T is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat. |
|||
Flexural Strength | 41.0 MPa | 5950 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MB006HS PP (Asia Pacific) LNP* Thermocomp* MB006HS is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Strength | 41.0 MPa | 5950 psi | ISO 178 |
Styrolution Polystyrol 454 C GR 2 PS Description: Polystyrol 454 C is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.Applications: TV-front panels and back covers, VCR fronts.. |
|||
Flexural Strength | 41.0 MPa | 5950 psi | ISO 178 |
Styrolution PS 454N HIPS Styrolution PS 454N is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.Good balance of toughness, high flow, and heat resistanceHigh gloss.. |
|||
Flexural Strength | 41.0 MPa | 5950 psi | ASTM D790 |
Stratasys® ABS ABS is a strong, durable production-grade thermoplastic used across many industries. ABS is an ideal material for conceptual prototyping through design verification through direct digital manufactur.. |
|||
Flexural Strength | 41.0 MPa | 5950 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MFB71L PP LNP* THERMOCOMP* MFB71L is a compound based on Polypropylene resin containing 35% Glass Bead, 5% Glass Fiber. Added features of this material include: Low Extractible. |
|||
Flexural Strength | 41.0 MPa | 5950 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MFB71L PP (Asia Pacific) LNP* Thermocomp* MFB71L is a compound based on Polypropylene resin. Added features of this material include: Low Extractible. |
|||
Flexural Strength | 41.0 MPa | 5950 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Flexural Strength | 41.0 MPa | 5950 psi | ASTM D790 |
Goodfellow TPX® DX350 Coating/Extrusion Grade Polymethylpentene This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a.. |
|||
Flexural Strength | 41.0 MPa | 5950 psi | ASTM D790 |
Lubrizol ESTALOC® 60204 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro.. |
|||
Flexural Strength | 41.0 - 55.0 MPa | 5950 - 7980 psi | Polypropylene; ASTM D790M |
DSM Somos® 9120 The need for movable parts is a constant when it comes to prototyping. Being able to ensure the proper fit for parts within a component can save both time and money. Somos® 9120 creates semi-transp.. |
|||
Flexural Strength | 41.0 MPa | 5950 psi | ASTM D790 |
Entec Hypro™ PPC-CC40 Natural Copolymer Polypropylene, 40% Calcium Carbonate Filled Information provided by Entec |
|||
Flexural Strength | 41.0 MPa | 5950 psi | ASTM D790 |
Entec Hypro™ PPH-CC30 Natural Homopolymer Polypropylene, 30% Calcium Carbonate Filled Information provided by Entec |
|||
Flexural Strength | 41.0 MPa | 5950 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0334M10CL Mica Reinforced Coupled |
|||
Flexural Strength | 41.0 MPa | 5950 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0334M20L Mica Reinforced |
|||
Flexural Strength | 41.0 MPa | 5950 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp CI001 PS (Asia Pacific) LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pa.. |