Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 393 MPa | 57000 psi | |
Pyrotek TS-111 Thermoset Electrical Insulation Product (Nema Grade: G-11) Glass reinforcement, Epoxy Resin, Natural Color. Good electrical and mechanical properties.ApplicationsSuperstructure support pads Bus bar insulators Pot cradle insulators Exhaust duct insulators M.. |
|||
Flexural Strength | 393 MPa | 57000 psi | |
MTI ThermoStran® TPU-60G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Flexural Strength | 393 MPa | 57000 psi | ASTM D790 |
Techmer ES HiFill® PA4/6 CF40 IM HS 40% Carbon Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites.. |
|||
Flexural Strength | 393 MPa | 57000 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP QC006 PA 6/10 (Asia Pacific) LNP* THERMOCOMP* QC006 is a compound based on Nylon 6/10 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 393 MPa | 57000 psi | ISO 178 |
SABIC Innovative Plastics LNP VERTON UV00AS PPA (Asia Pacific) LNP* Verton* UV00AS is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Strength | 393 MPa | 57000 psi | ISO 178 |
SABIC Innovative Plastics LNP VERTON UV00ASU PPA LNP* VERTON* UV00ASU is a compound based on Polyphthalamide resin containing 50% Long Glass Fiber. Added features of this material include: UV Stabilized, Heat Stabilized, Structural. |
|||
Flexural Strength | 393 MPa | 57000 psi | ASTM D790 |
Lubrizol Isoplast® 101LGF60NAT Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Flexural Strength | 393 MPa | 57000 psi | ASTM D790 |
Lubrizol ISOPLAST™ 2560 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaAvailableInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Flexural Strength | 393 MPa | 57000 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP PX01658 PA 6 LNP* Thermocomp* PX01658 is a compound based on Nylon 6 containing Proprietary Fillers. |
|||
Flexural Strength | 393 MPa | 57000 psi | ISO 178 |
SABIC Innovative Plastics LNP VERTON UV00AS PPA LNP* VERTON* UV00AS is a compound based on Polyphthalamide resin containing 50% Long Glass Fiber. Added features of this material include: Heat Stabilized, Structural. |