Mechanical Properties Metric English Comments
Flexural Strength 62.7 MPa
9090 psi
1.3 mm/min; ASTM D790
PolyOne LubriOne™ AT-000/18T 2S Acetal (POM) Copolymer
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Flexural Strength 62.7 MPa
9100 psi
ASTM D790
Polymer Resources PC/TP-GP3-IM PC/Polyester Alloy, Impact Modified
Superior Chemical Resistance, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide..
Flexural Strength 62.7 MPa
9100 psi
ASTM D790
Ravago Manufacturing Americas Enviramid™ N2300THL BK/HF Post Consumer Recycle Nylon 6
Impact Modified, High Flow, Heat Stabilized, Lubricated, Black and Made from EnViramid Post Consumer Recycled NylonInformation provided by Ravago.
Flexural Strength 62.7 MPa
9090 psi
ASTM D790
PolyOne Geon™ SF M7000 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Strength 62.7 MPa
9090 psi
ASTM D790
PolyOne Geon™ SF M7010 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Strength 62.7 MPa
9090 psi
ASTM D790
PolyOne Geon™ SF M7020 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Strength 62.7 MPa
9100 psi
ASTM D790
Techmer ES Electrablend® HIPS
Availability: North AmericaForms: PelletsFeatures: ConductiveInformation provided by TP Composites, Inc.
Flexural Strength 62.7 MPa
9100 psi
ASTM D790
Techmer ES Statiblend® HIPS C BK
Availability: North AmericaForms: PelletsFeatures: ConductiveAppearance: BlackTPCI# 7576148Information provided by TP Composites, Inc.
Flexural Strength 62.7 MPa

@Thickness 3.17 mm
9100 psi

@Thickness 0.125 in
ASTM D790
Samsung Cheil Industries Starex® SR-0340M High Heat Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Strength 62.7 MPa

@Thickness 3.17 mm
9100 psi

@Thickness 0.125 in
ASTM D790
Samsung Cheil Industries Starex® SR-0340M High Heat Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Strength 62.7 MPa
9100 psi
ASTM D790
Techmer ES HiFill® HDPE GF40 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightInformation provided by TP Composites, Inc.
Flexural Strength 62.7 MPa
9100 psi
ASTM D790
Techmer ES Luriblend® ABS TL2
Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
Flexural Strength 62.7 MPa
9100 psi
ASTM D790
Chesterton ARC SD4i High temperature ceramic reinforced erosion resistant coating
Description: An advanced ceramic composite for resurfacing and protection of metal surfaces in immersion service. It is normally applied in a thickness range of 250-370 microns (10-15 mils) per coat..
Flexural Strength 62.7 MPa
9100 psi
ASTM D790
Chesterton MRS SD4i Metal Rebuilding System
An advanced ceramic composite for resurfacing and protection of metal surfaces in immersion service. It is normally applied in a thickness range of 250-370 microns (10 – 15 mils) per coat. Non-shri..
Flexural Strength 62.7 MPa
9100 psi
Abatron AboCast 8503-6/AboCure 8503-6 Colorless Epoxy
AboCast 8503-6/AboCure 8503-6 is a slow hardening, colorless epoxy casting compound with low viscosity used for larger castings. It allows for large castings and offers low viscosity for bubble-free..
Flexural Strength 62.7 MPa
9100 psi
ASTM D-790
Axiall Suprel® SVA 9301 Rigid PVC, Molding
Georgia Gulf Suprel® SVA 9301 is a general purpose injection molding alloy with mid-range properties, providing a balance of impact strength and stiffness and featuring excellent UL flammability li..
Flexural Strength 62.7 MPa
9100 psi
ASTM D790
Techmer ES Luriblend® ABS TL10
Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.