Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Strength = 6700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 46.2 MPa
6700 psi
Perpendicular
Momentive Performance Materials BNC2 Boron Nitride (BN) Refractory Composite
Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mu..
Flexural Strength 46.2 MPa
6700 psi
ASTM D790
Techmer ES HiFill® PA6 L N MB (Conditioned)
Availability: North AmericaForms: PelletsAdditive: Lubricant and Nucleating AgentFeatures: Lubricated, Fast Molding Cycle, Good Processability and NucleatedTPCI# 7964102Information provided by TP Co..
Flexural Strength 46.2 MPa
6700 psi
ASTM D790
Techmer ES HiFill® PA6 LE BK (Conditioned)
Availability: North AmericaForms: PelletsAdditive: Lubricant and Nucleating AgentFeatures: Lubricated, Fast Molding Cycle, Good Processability, Low Extractables and NucleatedAppearance: BlackTPCI# 7..
Flexural Strength 46.2 MPa
6700 psi
ASTM D790
Total PSC 524B Polystyrene
Polystyrene 524B is a general purpose crystal polystyrene targeted for gloss coextrusion cap applications. It is specially formulated to reduce die buildup and die lines.Information provided by Tota..
Flexural Strength 46.2 MPa
6700 psi
ASTM D790
Total PSI 940E Impact Polystyrene
Description: 940E is a super high impact polystyrene designed for high gloss sheet extrusion and thermoforming applications that require additional toughness.Applications: The combination of high gl..
Flexural Strength 46.2 MPa
6700 psi
5 lb Core, 6 hrs @ 220°F, Vacuum Bag
Zyvex Performance Materials Aroply™ 250 Nano-Engineered Composite Film Adhesive
Aroply™ 250 Film Adhesive is a versatile, heat curing carbon-nanotube modified epoxy structural film adhesive available in a variety of film weights on a supported knitted nylon carrier. Cured adhe..
Flexural Strength 46.2 MPa
6700 psi
ASTM D790
Total PSI 825 Polystyrene
Polystyrene 825 is a high impact polystyrene for injection molding. They polymers ability to be molded on fast cycles with minimal stresses results in outstanding impact retention.Applications such ..
Flexural Strength 46.2 MPa
6700 psi
ASTM D790
Adell RQ-16 Copolymer Polypropylene, 30% Mica Reinforced
Data provided by Adell Plastics, Inc.
Flexural Strength 46.2 MPa
6700 psi
ASTM D790
M. Holland Company IS200 Polystyrene, High Impact  (discontinued **)
Uses: Audio Tapes, Household Goods, ToysProcessing Method: Injection MoldingInformation provided by M. Holland.
Flexural Strength 46.2 MPa
6700 psi
ASTM D790
Quadrant EPP Quadrant CPVC - ASTM D1748, Cell Classification (ASTM Product Data Sheet)
Copyright © lookpolymers.com All Rights Reserved