Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Strength = 68.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 68.3 MPa
9910 psi
1.3 mm/min; ASTM D790
PolyOne LubriOne™ 5209 FPL 20 Natural Acetal (POM) Copolymer
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Flexural Strength 68.3 MPa
9910 psi
1.3 mm/min; ASTM D790
PolyOne LubriOne™ AT-000/20T Black Acetal (POM) Copolymer
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Flexural Strength 68.3 MPa
9910 psi
ASTM D790
PolyOne Novablend™ 9562 Polyvinyl Chloride Alloy (PVC Alloy)
Custom MoldingInformation provided by PolyOne
Flexural Strength 68.3 MPa
9900 psi
ASTM D790
Ravago Manufacturing Americas Hylon® N1000STHL UV2 Nylon 6/6  (discontinued **)
Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Good Toughness, Lubricated, Heat StabilizedRoHS CompliantAuto Specifications: GM GMP.PA66.074 Color: BlackF..
Flexural Strength 68.3 MPa
9900 psi
after 16 hours in 50°C water
Malvern Minerals Nylon with Novakup® L-337 Silane-Treated Quartz Filler
Product data demonstrates the effect of the Novakup® (lamellar quartz surface treated with A-1100) filler. A separate entry demonstrates the effect of untreated Novacite® filler in nylon. Th..
Flexural Strength 68.3 MPa
9900 psi
90°; ASTM D790
Zyvex Performance Materials Arovex™ 180 Carbon Nanotube Strengthened Prepreg
Arovex® 180 Prepreg is a 180°F (82°C) curing carbon nanotube strengthened epoxy prepreg suitable for numerous composites applications. Arovex 180 resin contains an optimum level of carbon nanotub..
Flexural Strength 68.3 MPa
9900 psi
Machine; IPC TM-650 2.4.4
Arlon AD1000 PTFE/Woven Fiberglass/Ceramic Filled Laminate for Microwave Printed Circuit Boards
Only Woven Glass Reinforced PTFE/Ceramic with Dk of 10.2 or greaterHigh Copper Peel Strength allows for thinner etched line widthsLowest insertion loss availableLarger Panel sizes availableLow moist..
Copyright © lookpolymers.com All Rights Reserved