Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 70.33 MPa | 10200 psi | |
Abatron AboCast 8-7/Abocure 8-7 Epoxy
(discontinued **) 2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 1 lb. (2.2 kg): 125 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F)... |