Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 800 MPa | 116000 psi | Bending Strength; Double-Ring (40 mm/20 mm); 0.63 mm; DIN EN 1288 |
CeramTec Rubalit® HSS Alumina, 75% (High Strength Substrate) Rubalit® HSS (High Strength Substrate) displays the successful union of elasticity and strength. The ultrafine microstructure of Rubalit® HSS is the basis for its outstanding substrate surface qua.. |
|||
Flexural Strength | 800 - 1000 MPa | 116000 - 145000 psi | Longitudinal |
Goodfellow Carbon/Vinyl Ester Rod Carbon Fiber - Vinyl ester MatrixInformation provided by Goodfellow. |
|||
Flexural Strength | 800 - 1000 MPa | 116000 - 145000 psi | Longitudinal |
Goodfellow Carbon/Vinyl Ester Tube Carbon Fiber - Vinyl ester MatrixInformation provided by Goodfellow. |