Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 61.9 MPa | 8980 psi | ASTM D790 |
PolyOne Geon™ HTX Ultra LA426 Gray 2382 Polyvinyl Chloride Alloy (PVC Alloy) Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical propert.. |
|||
Flexural Strength | 61.9 MPa | 8980 psi | 20 x 40 mm |
CeramTec GRADE A LAVA Machinable Ceramic GRADE A LAVA is a machineable ceramic that exhibits good electrical and heat resistance. It is excellent in applications where close tolerances must be held. This material is available in a variety .. |