Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Yield Strength = 115 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 115 MPa
16700 psi
Epoxy Novolac 27%, Carbon fabric 73%
Epoxy Novolac - Dow Chemical "DEN 438". Carbon fabric - "VCA"
Compressive Yield Strength 115 MPa
16700 psi
DIN EN ISO 604
Wolf Kunststoff ZEDEX® ZX-750V5T A9T Polymer Alloy
Main Characteristics: Hard; Stiff; Tough; High dimensional stability; High fatigue strength; High weather resistance; Good fire behavior; Suitable for vacuum; Good machinability; Contains PTFE; Stre..
Compressive Yield Strength 115 MPa
16700 psi
Typical averaged test results for Abatron Adhesive/Casting Resins.
Abatron AboWeld 48-14/AboCure 48-14 Adhesive/Casting Resin
Information provided by Abatron, Inc. Adheres to metal, glass, ceramics, wood, masonry, etc. Material properties are based on a 2/1 mix ratio. Resin is white, curing agent is black. Gray blend a..
Compressive Yield Strength 115 MPa
16700 psi
Typical averaged test results for Abatron Adhesive/Casting Resins.
Abatron AboWeld 48-8/AboCure 48-8 Adhesive/Casting Resin
Information provided by Abatron, Inc. Adheres to metal, glass, ceramics, wood, masonry, etc. Material properties are based on a 2/1 mix ratio. Resin is white, curing agent is black. Gray blend a..
Compressive Yield Strength 115 MPa
16700 psi
Typical averaged test results for Abatron Adhesive/Casting Resins.
Abatron AboCast 37-10/AboCure 37-10 Adhesive/Casting
Information provided by Abatron, Inc. Adheres to metal, glass, ceramics, wood, masonry, etc. Material properties are based on a 2/1 mix ratio. Resin is white, curing agent is black. Gray blend a..
Compressive Yield Strength 115 MPa
16700 psi
Typical averaged test results for Abatron Adhesive/Casting Resins.
Abatron AboCast 45-10/AboCure 45-10 Adhesive/Casting
Information provided by Abatron, Inc. Adheres to metal, glass, ceramics, wood, masonry, etc. Material properties are based on a 2/1 mix ratio. Resin is white, curing agent is black. Gray blend a..
Compressive Yield Strength 115 MPa
16700 psi
Typical averaged test results for Abatron Adhesive/Casting Resins.
Abatron AboCast 53-15/AboCure 53-15 Adhesive/Casting
Information provided by Abatron, Inc. Adheres to metal, glass, ceramics, wood, masonry, etc. Material properties are based on a 2/1 mix ratio. Resin is white, curing agent is black. Gray blend a..
Copyright © lookpolymers.com All Rights Reserved