Mechanical Properties Metric English Comments
Compressive Yield Strength 138 MPa
20000 psi
10% Def.; ASTM D695
Quadrant EPP Ketron® CM HPV PEEK Polyetheretherketone; PTFE, Graphite, and Carbon Fiber Filled Bearing Grade, compression molded (ASTM Product Data Sheet)
Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to hot water or steam
Compressive Yield Strength 138 - 255 MPa
20000 - 37000 psi
Average value: 179 MPa Grade Count:6
Overview of materials for Nylon 66, Glass/Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of..
Compressive Yield Strength 138 MPa
20000 psi
ASTM D256
Techmer ES Electrafil® J-1/CF/30/TF/15 Nylon 66, 30% Carbon Fiber Reinforced, PTFE Lubed
Carbon Fiber Reinforced, PTFE Lubricated
Compressive Yield Strength 138 MPa

@Strain 1.00 %
20000 psi

@Strain 1.00 %
ASTM D695
Saint-Gobain Fluoroloy® A22 High Performance Seal Material
High modulus with excellent high-temperature resistance; Abrasion resistant; Chemically Inert; Recommended for back-up rings and for special applications. Information provided by Saint-Gobain P..
Compressive Yield Strength 138 MPa
20000 psi
at 8% compression
Zircar Refractory Composites RS-DR Refractory Sheet
TYPE RS-DR is a rigid pre-fired sheet that has been heat-treated to remove all organic binder and is stable to moisture attack. Refractory Sheet Type RS-DR is suited for use as a setter or barrier f..
Compressive Yield Strength 138 MPa
20000 psi
ASTM D695
Adell BR-14 Nylon 6, 20% Glass Reinforced
Data provided by Adell Plastics, Inc.
Compressive Yield Strength 138 MPa
20000 psi
ASTM D695
Adell BR-34 Nylon 6, 20% Glass Reinforced
Data provided by Adell Plastics, Inc.
Compressive Yield Strength 138 MPa
20000 psi
ASTM D695
Adell AJ-14 Nylon 66, 20% Glass Reinforced; High Impact
Data provided by Adell Plastics, Inc.
Compressive Yield Strength 138 MPa
20000 psi
ASTM D695
Adell AJ-34 Nylon 66, 20% Glass Reinforced; High Impact
Data provided by Adell Plastics, Inc.
Compressive Yield Strength 138 MPa
20000 psi
Max load under tribological use
Saint-Gobain Rulon® FCJ Grade Bearing/Seal PTFE  (discontinued **)
Saint Gobain Rulon® CJ is now produced as a part of the TriStar Plastics Corp. product line under the CJ Bearings trade name.Description: Rulon® is the Saint-Gobain trade name for their family of ..
Compressive Yield Strength 138 - 179 MPa
20000 - 26000 psi
Average value: 153 MPa Grade Count:12
Overview of materials for Diallyl Phthalate (DAP), Cast, Mineral Filler
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP), Cast, Mineral Filler". Each property range of values reported is minimum and ma..
Compressive Yield Strength 138 MPa
20000 psi
ASTM D695
Sumitomo Bakelite North America RX® 1-510N Mineral Filled Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ..